And what color were the pads that did not solder?
Were they a dull gray color or gold?
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paymon Sani
Sent: Friday, October 10, 2008 5:47 AM
To: [log in to unmask]
Subject: Re: [TN] PCB pad non-wetting issues
getting back to John, we ran 20 bare boards through wave and only wave
process and 2 boards exhibited this condition.
Regards,
Paymon
-----Original Message-----
From: Tan Geok Ang [mailto:[log in to unmask]]
Sent: October 9, 2008 9:23 PM
To: TechNet E-Mail Forum; Paymon Sani
Subject: RE: [TN] PCB pad non-wetting issues
The question is why it only happened on the solder side pads (believed
that solder flow through PTH barrel and fillets formed on the
component/top side of the board). Either black pad issue on the solder
side or the wetting/contact time is too long at wave soldering process.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paymon Sani
Sent: Thursday, 9 October 2008 10:54 PM
To: [log in to unmask]
Subject: Re: [TN] PCB pad non-wetting issues
No, this is a good suggestion. I will propose it based on the PCB
pricing and failure rate.
Thank you,
Paymon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: October 9, 2008 10:25 AM
To: [log in to unmask]
Subject: Re: [TN] PCB pad non-wetting issues
Have you tried running a bare board through to confirm/eliminate the
heating
cycles?
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paymon Sani
Sent: Thursday, October 09, 2008 6:57 AM
To: [log in to unmask]
Subject: [TN] PCB pad non-wetting issues
Hello All,
We are experiencing a pad non-wetting issue for the though-hole
component pads ONLY! The PCB goes through few heat cycles with top and
bottom side assembly during at SMT process and then through-hole
assembly at wave process. The problem is found at Wave process. The Pb
solder does not wet to the through-hole component pads on the solder
side only! An SEM/EDS evaluation revealed high concentration of P in the
Nickel and Nickel/Tin intermetalic layer of 11% to 21%. I would like to
ask anyone if they have experienced a similar defect in the past. What
is the Root Cause?
Thank you in advance,
Paymon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
__________ NOD32 3475 (20080926) Information __________
This message was checked by NOD32 antivirus system.
http://www.eset.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
__________ NOD32 3475 (20080926) Information __________
This message was checked by NOD32 antivirus system.
http://www.eset.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|