Hi Leo & Paul,
With Pb-free, you need to consider Td, Tg and CTE for reliability in
combination---that is why I developed the STII (Soldering Temperature Imact
Index)-parameter.
Also, you also need to consider that you get different CTE's in the x and
-direction (about 2 ppm/C), not to say anthing about the diagonal.
Werner
**************
It's only a deal if it's where you want to go. Find your travel
deal here.
(http://information.travel.aol.com/deals?ncid=aoltrv00050000000047)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------