Well, I've always wanted to be more Wilson than Tim, if I could be 1/2
and 1/2 I'd be a happy guy.
Besides, he'd approve of a big induction heater... The Binford 5000
solder machine, I'm sure there was one in his basement. I'll have to
get one that runs on 220v though, for more power...
regards,
- Graham
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dwight Mattix
Sent: Friday, September 05, 2008 3:29 PM
To: [log in to unmask]
Subject: Re: [TN] Wire Harness question - soldering 0 AWG wire?
...as Tim Allen weeps...
At 08:20 AM 9/5/2008, Graham Collins wrote:
>I think I'll pass on the open flame concepts... I do need to be able
>to ship this afterall...
>
>
>regards,
> - Graham
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
>Sent: Friday, September 05, 2008 12:15 PM
>To: [log in to unmask]
>Subject: Re: [TN] Wire Harness question - soldering 0 AWG wire?
>
>Now that's what I'm talking about. Torch that sucker!
>
>Happy Firday,
>
>KennyB
>
>-----Original Message-----
>From: Dwight Mattix [mailto:[log in to unmask]]
>Sent: Thursday, September 04, 2008 6:50 PM
>To: [log in to unmask]
>Subject: Re: [TN] Wire Harness question - soldering 0 AWG wire?
>
><http://www.ptsconline.com/services/blowtorch.jpg>more power. heh,
>heh,heh
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>or
>(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>archives of previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
>per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|