Trikeman,
I've solved the problem dreamporarily by means of a temporarily and temperaturearily solution. Woke up suddenly at midnight, had just fallen asleep. Something pinged to my brain: pssst...your Black&Decker amateur heat gun ...psssst. I stood up, went to the garage and found my cheap and well used heatgun. Put it in my rucksack (use my old Yamaha Virago 1100 XV to the job when it's fine weather). With large package in a jaw, Hydrox superflux richly applied, temperature probe attached, I could obtain the most beautiful solder joints. Maximum approx. +300 C during about 1 minute, flowing more Hydrox in order to protect against nickel oxidizing. So, today I've fixed a professional heatgun with many nossles, a good temperature probe and am going to shop a fixture so that you can rotate the package and solder each side separately. The secret is to have the soldering done with coaxes and feedtrues standing upright AND using lots of Hydrox.
We have exactly same SST. Good idea, will spend some thinking on your proposal. AuSn...hmmm...to bright Nickel...hmmm...lots of hmmmmmm...
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Creswick, Steven
Sent: den 25 september 2008 12:32
To: [log in to unmask]
Subject: Re: [TN] Soldering SMA to heavy RF packages, need advice
Inge,
I have used the SST vac/pressure reflow system for criters similar to this. Here is their web site - http://www.sstinternational.com/prod_3130.html
The cost back then was ~$150K. Not sure what they are up to now.
The base unit had the capability of 50-100mT vacuum, or 2-3 atm of pressure [gas of your choice] and all points in between. Programmable rise, hold and fall rates [within reason], multiple gas flows and rates.
You likely saw a very small sample of some of the high lead and Au/Sn with LTCC configurations permitted with this equipment.
Heating of components is accomplished by conduction from graphite tooling plates - the tooling plates being heated by passage of electric current within a sealed chamber.
On my unit, I could not plumb in more [more concentrated] than a forming gas [5-6% hydrogen], however. That might be barely suitable for oxidized nickel [we never used fluxes inside the chamber] if you can get the temperatures high enough [if your components can withstand them] to actually activate the hydrogen's reduction effect. At 300-400°C, or below, a good clean nitrogen appears to work just as well from a practical experience standpoint.
You have left out a lot of details, possibly the nature of the beast at this point, however. Are you dealing with matched, or compression seals? Have a clue for what the max temp capabilities are so that a reflow hierarchy can be established?
Doesn't sound like you could use 280°C Au/Sn eutectic very will with the possibility of oxidized Ni, but it just may work if you can clean things up well prior to reflow. My assumption is that you desire something stronger/better than Sn/Ag eutectic, or generic hi-temp lead bearing alloys.
In theory the newer SST's [1000°C max temp capability] can handle the generic Cu/Ag eutectic at ~780°C, but I did not have the opportunity to go that high.
When using the Cu/Ag eutectic, the Kyocera's & NTK's of the world seemed to always go to the cracked ammonia atmosphere tunnel kilns. I never got to play with the 25% hydrogen atmosphere, like the 'big boys'.
Corporate had an 'Astro' batch furnace that could get there, however.
There are various other 'active braze' alloys containing titanium that will fire in these temperature ranges, but I believe they will like to be in the cracked ammonia environment as well.
Lastly, if you believe the advertising [I have some swamp land to sell, if you do] you could buy some epoxy and make a "hermetic" seal !! - just kidding.
You come up with all the fun stuff!
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Wednesday, September 24, 2008 10:26 AM
To: [log in to unmask]
Subject: [TN] Soldering SMA to heavy RF packages, need advice
TNetters godday.
Target is very large metal packages with bright nickel finish. Imagine soldering hermetic feedtrues. Nickel needs higher temperature and longer exposure time than copper, silver, gold and other metals. Vapour phase soldering is maximum 218 Centigrades, which I believe is not high enough. Iron soldering is not practical for launches. IR oven could be an idea if we add protection gas. Hot gas stations (Nitrogen)seem to be too lame. Resistance soldering not tested, unknown for SMA. Torch heard of, ought to be impractical, will burn flux and miscolor package. Laser soldering not practised.
Anyone out there with experience from this kind of soldering?
Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. [gntx v.1]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|