TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bob METCALF <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bob METCALF <[log in to unmask]>
Date:
Wed, 24 Sep 2008 17:09:19 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (83 lines)
More and more people are going to Nickel, Palladium, Gold as the preferred 
surface for gold wire bonding. 

Regards,

Bob Metcalf
Atotech Western Regional Manager

Cell 714-334-7667
E-Mail [log in to unmask] 

This e-mail and any attachments hereto are business documents of Atotech 
USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS INFORMATION. 
Unauthorized disclosure and/or use of information contained in this email 
is prohibited. If you are not the intended recipient, you may not read, 
use, disseminate or copy this message or any other files transmitted with 
it. 



Anand Paliwal <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
09/24/2008 12:07 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Anand Paliwal <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Plating types






Hi all,
i am quite new to this community so pls help me.

What is the Difference between ENIG and Soft gold wire Bondable Plating  ?

is the ENIG type of plating for soft wire bondable ?

i have COB on board so i want to specify  Soft Gold wire bondable plating 
but 
my fab house gives ENIG.


Pls reply 

Thanks

Anand 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2