You are absolutely right, Mark, thanks for the correction.
Inge
----- Original Message -----
From: "Woolley, Mark D. (Mark)" <[log in to unmask]>
To: "TechNet E-Mail Forum" <[log in to unmask]>; "Inge"
<[log in to unmask]>
Sent: Monday, September 15, 2008 9:50 AM
Subject: RE: [TN] qualification of manual bench cleaning processes
Inge,
Ethylene is a vapor at -100C. Could it be ethyl alcohol (Ethanol) or
isopropyl alcohol (2-propanol) used to clean the PWBs. Both would be
compatible with the Acetone rinse afterwards as you indicated.
mark
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Saturday, September 13, 2008 2:08 PM
To: [log in to unmask]
Subject: Re: [TN] qualification of manual bench cleaning processes
Seven times!! What heaven of flux or soldering process do you use?
Something
must be very wrong!
We run our boards, independent of if they are SnPb solderd or Leadfree
soldered, independent on what flux is used and independent on what
boards
are used, through a tunnel washer with Vigon 200 as agent. We have done
that
for years without seeing any residues. Yes, there are some parts that
are
not allowed to go through that process, e.g. hybrids. They are hand
cleaned
in tanks filled with 60 Centigrades warm etylene, warm Aceton and
finally
rinsed in DI. Three step with other words.
Inge
----- Original Message -----
From: "Gervascio, Thomas" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, September 13, 2008 12:14 PM
Subject: [TN] qualification of manual bench cleaning processes
We have in the past abandoned manual defluxing after hand soldering
(ROL0 and ROM0) rosin fluxes with in line saponified washes. Well in
some cases we have to run boards seven times through the in line wash
resulting in degraded anodized finish, part marking removal , etc. I am
trying to gather the experiences and methodoloy to select the best type
of manual defluxing processes and qualify to make sure that the process
is adequate and any residues would be benign. Would start with the
J-STD-001 cleaning process qualification testing on materials and
residues but was trying to see what other folks are using out there
rather than being bombarded with sales pitches.
Any experiences and information would be appreciated.
Tom
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|