Good evening from Spain.
The problem we have is the following. After soldering, we conformal coating a
class 3 polyamide board (blind vias) with Parylene C. Until this moment, all is
OK.
Then, the board pass the ESS -thermal cycling-, and it is at this moment
when appears a halo around the solder joints. The test tape performed in that
area fails. I’ll send some pictures to Steeve Gregory for reference.
We have coated at the same time (and processed in the same conditions,
that is soldering, cleaning…) the “suspicions” polyamide boards with other type
of boards (polyamide & rigid). We only obtain negative results with the first
ones.
We have sent some boards to an external lab for FTIR testing, and we are
waiting for the final results.
Our though is that cause of the problem is the PCB, but we need to
demonstrate it. It's like some contaminant appears under the conformal
coating caused by the temperature (from the inner layers of the PCB?)
So, what we need is that somebody turns the ”light” on.
Thank you for your help.
Juan T. Marugán López
Supply Chain Management
Indra Sistemas SA (Spain)
[log in to unmask]
www.indra.es
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|