Thanks Phil but no luck with the industrial Sharpie. That's what we are
currently trying to use and it washes right off with IPA.
I did some searching on the web and made a few phone calls. What it's
sounding like is that thanks to all the "do gooders" they have had to change
the formulas in the paint pens to where they don't dry very fast. I guess
too many kids were sucking the trichlor out of them ;-)
I did find one company that is sending me a sample of the Sharpie Paint pen.
I'll update this post once I get it and put it through its paces.
Have a great weekend! Here on beautiful Whidbey Island in Washington State I
know I will.
KennyB
-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Friday, September 05, 2008 5:13 AM
To: TechNet E-Mail Forum; Ken Bloomquist
Subject: RE: [TN] Marking Question
Ken
Sharpie makes an "Industrial" version that I have used. It is claimed to
stay on even through 500° F steam and most solvents. An alternative is some
of the paint pens. The brand escapes me right now, but there are at least
two major name manufacturers that make a pen with paint or epoxy ink.
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|