Hi Paul!
Have your *.AVI posted. It's at:
http://stevezeva.homestead.com/files/Dendritic_Growth.avi
Creating dendritic growth is pretty simple and doesn't take much time at
all. Get a scrap board and find an area with two parallel traces. Scrape
the mask off a section of the traces and then attach a 9-volt battery to
the traces at a via or PTH. Just like Paul said, put a drop of water on
the traces and you'll have dendrites in just a couple of minutes if that
long...
Steve
-----Original Message-----
From: Paul Reid [mailto:[log in to unmask]]
Sent: Wednesday, September 03, 2008 9:06 AM
To: TechNet E-Mail Forum; Lum Wee Mei
Subject: RE: [TN] Video on dendrite growth
Hi Wee,
I have a short animation I created showing the dendritic growth I
observed on boards with surface contamination. I have ask Steve if he
would post it for down load.
The animation is of a drop of distilled water between two adjacent pads.
Current is applied between the pads, there is out gassing followed by
dendritic growth.
Sincerely,
Paul Reid
Program Coordinator
PWB Interconnect Solutions Inc.
235 Stafford Rd., West, Unit 103
Nepean, Ontario
Canada, K2H 9C1
613 596 4244 ext. 229
Skype paul_reid_pwb
[log in to unmask] <mailto:[log in to unmask]>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lum Wee Mei
Sent: Tuesday, September 02, 2008 9:09 PM
To: [log in to unmask]
Subject: [TN] Video on dendrite growth
Hello,
Anyone of you have a video showing the dendrite growth to share?
Thanks and Regards,
~ Wee Mei ~
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|