Hi Bob,
Thanks for the info.
i confirmed from Fabricator they are actually doing Electrolytic Nickel and gold
plating so no need of Phosphurous.
As IPC Standard doesn't specify the thickness of Nickel and Gold for
Electrolytic plating Process it only specifies ENIG thickness..in 4552..?
Can i know if there is any standard Specifications for the Electrolytic Nickel,
Gold plating Thicknesses ?
Thanks for the reply.
Regards,
Anand
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------