Eric,
You are just kidding, right?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric CHRISTISON
Sent: Wednesday, September 24, 2008 10:35 AM
To: [log in to unmask]
Subject: Re: [TN] Soldering SMA to heavy RF packages, need advice
Inge,
Don't the people who designed this thing have some idea how it should be
soldered?
Regards,
Thayer, Wayne wrote:
> Hi Inge!
>
> Nickel is pretty lossy, so you could possibly heat with electrical
> energy. Still lots of current required--probably on the order of
> 100A/mm of nickel. Nickel doesn't conduct heat real well either, so
> you would want to drive the current pretty close to where the solder
> needs to be melted. I'll bet a few days of playing with an arc
> welding power supply would get you a process. Or you could just use a
> car battery and some jumper cables and see what happens!
>
> Problem I see with this technique might be package warpage due to
> differential coeff of expansion and the local heat, similar to
> problems of using a torch, but the electrical would have much better
control.
>
> Wayne Thayer
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
> Sent: Wednesday, September 24, 2008 10:46 AM
> To: [log in to unmask]
> Subject: Re: [TN] Soldering SMA to heavy RF packages, need advice
>
> Mike,
>
> THAT was new to me! Good start, I'd say, many thanks. Hope our machine
> can manage 260 C.
>
> Inge
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Sewell
> Sent: den 24 september 2008 16:33
> To: [log in to unmask]
> Subject: Re: [TN] Soldering SMA to heavy RF packages, need advice
>
> Inge,
>
> Galden makes fluids that go to 260C...
>
> http://www.solvaysolexis.com/static/wma/pdf/9/7/7/0/Galden%20VPS.pdf
>
> Mike
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
> Sent: Wednesday, September 24, 2008 9:26 AM
> To: [log in to unmask]
> Subject: [TN] Soldering SMA to heavy RF packages, need advice
>
> TNetters godday.
>
> Target is very large metal packages with bright nickel finish. Imagine
> soldering hermetic feedtrues. Nickel needs higher temperature and
> longer exposure time than copper, silver, gold and other metals.
> Vapour phase soldering is maximum 218 Centigrades, which I believe is
> not high enough. Iron soldering is not practical for launches. IR oven
> could be an idea if we add protection gas. Hot gas stations
> (Nitrogen)seem to be too lame. Resistance soldering not tested,
> unknown for SMA. Torch heard of, ought to be impractical, will burn
> flux and miscolor package. Laser soldering not practised.
>
> Anyone out there with experience from this kind of soldering?
>
> Inge
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> This e-mail and any files transmitted with it may be proprietary and
are intended solely for the use of the individual or entity to whom they
are addressed. If you have received this e-mail in error please notify
the sender.
> Please note that any views or opinions presented in this e-mail are
solely those of the author and do not necessarily represent those of ITT
Corporation. The recipient should check this e-mail and any attachments
for the presence of viruses. ITT accepts no liability for any damage
caused by any virus transmitted by this e-mail.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
--
Eric Christison Msc
Mechanical Engineer
Consumer & Micro group
Imaging Division
STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom
Tel: +44 (0)131 336 6165
Fax: + 44 (0)131 336 6001
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|