Fabrice,
When I was evaluating X-Ray equipment, I brought precision ball bearings
(I think they were .050").
Each machine had some sort of measurement tool, but no matter the machine
or changing focus, tilting 50-75 degrees, etc., the .050" ball bearing was
my benchmark.
To stop the ball bearing from rolling around on the table or assembly, I
glued it to a small piece of conductive composite material (left-over wave
solder fixture stock).
Al Kreplick
Sr. Manufacturing Engineer
Circuit Card Assembly
Air-toAir/Precision Strike/Land Combat
Raytheon Integrated Defense Systems
978-470-9931office
978-245-1702 pager
978-470-4307 fax
[log in to unmask]
fabrice pires <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/09/2008 11:01 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
fabrice pires <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] precise void size measurement
Hi Techneters,
I would like your advices on the best way to calibrate XRay pictures in
aim to measure precisely voids inside BGA balls, after assembly.
Everyone should agree on the fact slight setup variation on XR equipment
could change significantly the void size results.
Do you have any trick to improve precision measures whatever the XR
equipment?
Does the use of any reference/calibration on boards exists in that aim?
Fabrice
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|