Mon, 29 Sep 2008 20:10:11 +0100
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (268 lines)
 
IPA can remove water sol fluxes but it's much better to use water, but water
won't look at resin as you say.
A semi-aqueous cleaner could remove both a water sol flux and resin, but
there could well be an interaction between the two fluxes during soldering
if used together which could lead to difficult to remove products or
initiate/increased rate of pyrolising leading to insoluble residues.  Hence
my comment about 'gruesome mixture' and question to know what is actually
being contemplated. 
[A high activity flux could just be a high solids RA rosin or an OA as you
say.]

Regards 

Mike 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, September 29, 2008 7:12 PM
To: [log in to unmask]
Subject: Re: [TN] HAL finished circuit boards

Thanks for answering my question, Roger, before it was even posted. 

Now, I'd like to know who qualified HAL (hot air leveled Sn, which I assume
is different from ISn). How was it qualified?

And getting back to the original question: "Is there any negative or
positive impacts of assembling HAL coated boards with some parts being tin
only using hand soldering with very active flux and 63/37 resin core
solder?"

To clarify, you are taking a circuit board with a tin-only finish, and you
are going to solder components also having a tin-only finish using a
resin-cored (to me resin-core means RMA or RA) Pb63Sn37 wire solder, and you
are going to use a "highly activated" benchtop flux to do the soldering,
which I would assume is a water-soluble OA flux. 

Then the answer is yes, you are going to have problems.

If you were going to solder this combination using a lead-free solder I
would say you are planting yourself a veritable garden from which millions
of tin whiskers could sprout. But you are not, you are using a leaded 63/37
solder, so my first inclination is that you should be OK from a whisker
standpoint, as the lead in the Sn63Pb37 wire solder should mitigate whisker
growth.

But when you speak of using what I assume is a highly active water soluble
liquid benchtop flux and mixing it with the RMA or RA flux residues from the
cored wire solder, then yes, you will have issues of cleanliness. Whenever
you mix those two, the ensuing mess is almost impossible to clean
completely. One reacts with water, the other reacts with alcohol.

Never the twain should mix.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, September 29, 2008 12:16 PM
To: [log in to unmask]
Subject: Re: [TN] HAL finished circuit boards

Explain to me the difference between Hot Air Solder Leveled (HASL) and Hot
Air Level (HAL). 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Connitt
Sent: Monday, September 29, 2008 11:56 AM
To: [log in to unmask]
Subject: Re: [TN] HAL finished circuit boards

Actually,
The boards are HAL, not HASL finish. At least that's what he told me..
I was just wondering if there could be any detrimental effects from
switching from HASL to HAL and use the same 63/37 resin core solder. I am
not too sure what he is using the flux for if the solder has flux in it
already. Just relaying information.
Dave Connitt 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Willis
Sent: Monday, September 29, 2008 12:44 PM
To: [log in to unmask]
Subject: Re: [TN] HAL finished circuit boards

If you have HASL Hot Air Solder Levelled boards and tin finish component and
they are both solderable why would you need to use a highly activated flux?

Any no clean product from many industry suppliers should work perfectly
well.

Many thanks, sorry to give a basic answer?

Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
 
www.ASKbobwillis.com
New Bob Willis "Printed Board Inspection & Quality Control Workshop"
24th March www.ASKbobwillis.com/faworkshops.pdf
 
"Troubleshooting Your Assembly Yields Workshop" 25th March
www.ASKbobwillis.com/faworkshops.pdf
 
Book Bob's "Step by Step Failure Analysis Workshop" 22nd April
www.ASKbobwillis.com/faworkshops.pdf
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: 29 September 2008 17:12
To: [log in to unmask]
Subject: Re: [TN] HAL finished circuit boards

".....very active flux and 63/37 resin core solder......."

Sounds gruesome mixture.

The impact: a rigorous cleaning procedure would be required What that would
be would depend on which very active flux and what type resin?


Regards 

Mike Fenner
Indium Corporation  


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Connitt
Sent: Monday, September 29, 2008 12:33 PM
To: [log in to unmask]
Subject: [TN] HAL finished circuit boards

Good Morning,
Is there any negative or positive impacts of assemblying HAL coated boards
with some parts being tin only using hand soldering with very active flux
and 63/37 resin core solder? An old customer asked me this over the weekend
and I thought I would forward the question to the list.
Thanks,
 
Dave Connitt CID+
Printed Circuit Designer
KDI Precision Products, Inc.
A Wholly Owned Subsidiary of:
L3 Communications
3975 McMann Road
Cincinnati, Ohio 45245
Ph. 513- 943-2010   Fax 513-943-2288

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient, please contact the
sender by return and delete the material from any computer.
Any review, retransmission, dissemination, or other use of, or taking of any
action in reliance upon this information by persons or entities other than
the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness.
Indium Corporation does not accept responsibility for changes made to this
email after is was sent.
Any opinions or recommendations expressed herein are solely those of the
author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2