TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 29 Sep 2008 13:09:17 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Stoops <[log in to unmask]>
Subject:
From:
Roger Stoops <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (191 lines)
In what way is HAL different from HASL?  Some use the difference to
distinguish between SnPb solder (HASL) and Pb-free solder (HAL).  Solder
is the only finish that I am aware of that utilizes hot-air leveling for
creating a fairly flat finish anyway, so it appears your concern would
be whether the finish is SnPb or Pb-free Sn.  Correct?

And to this, some component suppliers have been providing tin-only
finish on parts for years, most notably smd capacitors.  Using SnPb
solder on Sn boards and parts should work fine, assuming your assemblies
are not RoHS-compliant.  We (persons I work for) have had no problems so
far, don't anticipate any.

Besides semantics, in which your customer may be worrying about a
non-existent problem, me thinks Bob's analysis is correct.

Roger

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Connitt
Sent: Monday, September 29, 2008 12:56 PM
To: [log in to unmask]
Subject: Re: [TN] HAL finished circuit boards

Actually,
The boards are HAL, not HASL finish. At least that's what he told me..
I was just wondering if there could be any detrimental effects from
switching from HASL to HAL and use the same 63/37 resin core solder. I
am not too sure what he is using the flux for if the solder has flux in
it already. Just relaying information.
Dave Connitt 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Willis
Sent: Monday, September 29, 2008 12:44 PM
To: [log in to unmask]
Subject: Re: [TN] HAL finished circuit boards

If you have HASL Hot Air Solder Levelled boards and tin finish component
and they are both solderable why would you need to use a highly
activated flux?

Any no clean product from many industry suppliers should work perfectly
well.

Many thanks, sorry to give a basic answer?

Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
 
www.ASKbobwillis.com
New Bob Willis "Printed Board Inspection & Quality Control Workshop"
24th March www.ASKbobwillis.com/faworkshops.pdf
 
"Troubleshooting Your Assembly Yields Workshop" 25th March
www.ASKbobwillis.com/faworkshops.pdf
 
Book Bob's "Step by Step Failure Analysis Workshop" 22nd April
www.ASKbobwillis.com/faworkshops.pdf
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: 29 September 2008 17:12
To: [log in to unmask]
Subject: Re: [TN] HAL finished circuit boards

".....very active flux and 63/37 resin core solder......."

Sounds gruesome mixture.

The impact: a rigorous cleaning procedure would be required What that
would be would depend on which very active flux and what type resin?


Regards 

Mike Fenner
Indium Corporation  


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Connitt
Sent: Monday, September 29, 2008 12:33 PM
To: [log in to unmask]
Subject: [TN] HAL finished circuit boards

Good Morning,
Is there any negative or positive impacts of assemblying HAL coated
boards with some parts being tin only using hand soldering with very
active flux and 63/37 resin core solder? An old customer asked me this
over the weekend and I thought I would forward the question to the list.
Thanks,
 
Dave Connitt CID+
Printed Circuit Designer
KDI Precision Products, Inc.
A Wholly Owned Subsidiary of:
L3 Communications
3975 McMann Road
Cincinnati, Ohio 45245
Ph. 513- 943-2010   Fax 513-943-2288

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are
intended solely for the addressee(s) and may be legally privileged
and/or confidential. If you are not the intended recipient, please
contact the sender by return and delete the material from any computer.
Any review, retransmission, dissemination, or other use of, or taking of
any action in reliance upon this information by persons or entities
other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery,
and unauthorized alteration. This email has been prepared using
information believed by the author to be reliable and accurate, but
Indium Corporation makes no warranty as to accuracy or completeness.
Indium Corporation does not accept responsibility for changes made to
this email after is was sent.
Any opinions or recommendations expressed herein are solely those of the
author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2