More and more people are going to Nickel, Palladium, Gold as the preferred
surface for gold wire bonding.
Regards,
Bob Metcalf
Atotech Western Regional Manager
Cell 714-334-7667
E-Mail [log in to unmask]
This e-mail and any attachments hereto are business documents of Atotech
USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS INFORMATION.
Unauthorized disclosure and/or use of information contained in this email
is prohibited. If you are not the intended recipient, you may not read,
use, disseminate or copy this message or any other files transmitted with
it.
Anand Paliwal <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/24/2008 12:07 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Anand Paliwal <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Plating types
Hi all,
i am quite new to this community so pls help me.
What is the Difference between ENIG and Soft gold wire Bondable Plating ?
is the ENIG type of plating for soft wire bondable ?
i have COB on board so i want to specify Soft Gold wire bondable plating
but
my fab house gives ENIG.
Pls reply
Thanks
Anand
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|