TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Anand Paliwal <[log in to unmask]>
Date:
Wed, 24 Sep 2008 14:44:27 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Robin John <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Robin John <[log in to unmask]>
Parts/Attachments:
text/plain (59 lines)
ENiG is great for Al wire bonding. But you need 10-25 micro inches of
soft gold for gold wire bonding

Robin John

 
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Anand Paliwal
Sent: Wednesday, September 24, 2008 2:07 PM
To: [log in to unmask]
Subject: [TN] Plating types

Hi all,
i am quite new to this community so pls help me.

What is the Difference between ENIG and Soft gold wire Bondable Plating
?

is the ENIG type of plating for soft wire bondable ?

i have COB on board so i want to specify  Soft Gold wire bondable
plating but 
my fab house gives ENIG.


Pls reply 

Thanks

Anand  

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2