TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 18 Sep 2008 16:15:58 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Swanson <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Peter Swanson <[log in to unmask]>
Parts/Attachments:
text/plain (290 lines)
Gosh, darn... I knew I didn't put enough "it depends" in there.
 
Without getting to far into commercial specifics, I agree that older UV
coatings were more brittle, but newer UV coatings are tending to be more
resilient.
 
"Easy to rework" can mean "poor solvent resistance" - you will need to
balance these two requirements for your application. On the other hand,
if you specify resistance to all known solvents, all known temperatures
and all abrasion, then do not expect to ever be able to remove it!
 
Your mileage may vary.
Peter
 
________________________________

Peter Swanson	 [log in to unmask]	  
<http://www.intertronics.co.uk/adhere/index.htm> 	
INTERTRONICS, Oxfordshire, England 	Tel: +44 1865 842842	
INTERTRONICS <http://www.intertronics.co.uk/>  is dedicated to providing
quality material, consumable and equipment solutions to the high
technology, high performance assembly industries, incorporating
outstanding levels of technical support and customer service.	  	
Read the latest news <http://www.intertronics.co.uk/blog/blog.htm>  in
our blog!	  	
________________________________

 



________________________________

	From: [log in to unmask]
[mailto:[log in to unmask]] 
	Sent: 18 September 2008 15:58
	To: TechNet E-Mail Forum; Peter Swanson
	Subject: Re: [TN] NEW! DUAL-CURET 9481 ELECTRONIC CONFORMAL
COATING
	
	
	
	I would generally agree with Peter, but the degree of protection
is very much an "it depends" proposition.   We use 1B31 here and have
for a long time.  I did to evaluations of Dymax 984 a number of years
ago, and I am sure the 9481 has advanced from when I did that testing 7
years ago.   But one of the things that I found was that the material
was a blend of epoxy, acrylic, and urethane polymers.  It gave almost
bulletproof for chemical resistance, had excellent adhesion, but when we
did thermal cycling, we had lots of cracking and peeling around the -55C
and -65C extremes, a place where UV cures have historically had
problems.  We also found the material to be very hard to rework. 
	
	Again, I have not tested the 9481, but if you have to work in
worlds below -40C, or reworkability is important, then work that into
your evaluation plan. 
	
	Doug Pauls
	Rockwell Collins 
	
	
	
Peter Swanson <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]> 

09/18/2008 08:18 AM 
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Peter Swanson <[log in to unmask]>


To
[log in to unmask] 
cc
Subject
Re: [TN] NEW! DUAL-CURET 9481 ELECTRONIC CONFORMAL COATING

	




	Humiseal 1B31 is a single part, solvented acrylic coating, which
"dries"
	(solvent evaporation) fully in about 1-7 days at room
temperature,
	depending.  Solvented acrylic coatings are very popular and
widely used,
	in my experience.
	
	In general terms, you will get more robust protection from a
coating
	which fully cross-links, and this often means adding external
energy
	(heat or light, etc). 
	
	Selection of the optimal coating depends on a number of factors,
	including operating temperatures and working environments,
customer
	specifications, electrical characteristics, reworkability and
even
	production volumes and required process speed. No one coating is
	necessarily better than another; horses for courses.
	
	Regards,
	Peter
	
	--------------------------------------------------------
	Peter Swanson           [log in to unmask]
	INTERTRONICS                http://www.intertronics.co.uk
	Tel: +44 1865 842842                   Oxfordshire, England
	
	INTERTRONICS is dedicated to providing quality material,
consumable 
	and equipment solutions to the high technology, high performance

	assembly industries, incorporating outstanding levels of
technical 
	support and customer service.
	
	Read our news! http://www.intertronics.co.uk/blog/blog.htm
	
	-----Original Message-----
	From: Reuven Rokah [mailto:[log in to unmask]] 
	Sent: 18 September 2008 14:06
	To: TechNet E-Mail Forum; Peter Swanson
	Subject: RE: [TN] NEW! DUAL-CURET 9481 ELECTRONIC CONFORMAL
COATING
	
	Hi Peter,
	
	Can you compare it with the 1B31?
	
	Best Regards
	
	Reuven ROKAH
	e mail: [log in to unmask]
	P Think green before printing this mail... Thanks
	
	
	-----Original Message-----
	From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter
Swanson
	Sent: Thursday, September 18, 2008 11:40 AM
	To: [log in to unmask]
	Subject: Re: [TN] NEW! DUAL-CURET 9481 ELECTRONIC CONFORMAL
COATING
	
	DYMAX 9481 is a single part acrylated urethane conformal
coating. It has
	a secondary moisture cure mechanism (a bit like the cure
mechanism of a
	single part RTV silicone) for those areas which are in shadow to
light.
	The primary cure mechanism is still UV/visible light.
	
	Traditional UV acrylic conformal coatings had a secondary
thermal cure,
	so that's what makes this product new - if a secondary cure is
required,
	there is no need to add heat, the moisture cure just happens
over time.
	
	There are similar products from other vendors. This type of
chemistry is
	a valid choice to evaluate for your coating requirements, but
much
	depends on board geometry, application methods, requirements of
cured
	material, etc.
	
	Regards,
	Peter
	
	--------------------------------------------------------
	Peter Swanson           [log in to unmask]
	INTERTRONICS                http://www.intertronics.co.uk
	Tel: +44 1865 842842                   Oxfordshire, England
	
	INTERTRONICS is dedicated to providing quality material,
consumable and
	equipment solutions to the high technology, high performance
assembly
	industries, incorporating outstanding levels of technical
support and
	customer service.
	
	Read our news! http://www.intertronics.co.uk/blog/blog.htm
	
	-----Original Message-----
	From: TechNet [mailto:[log in to unmask]] On Behalf Of Leigh-Ann
Litavis
	Sent: 18 September 2008 01:10
	To: [log in to unmask]
	Subject: [TN] NEW! DUAL-CURE(tm) 9481 ELECTRONIC CONFORMAL
COATING
	
	Hi Technetters,
	
	Can anyone give me some information on this new Dynmax material?
Has
	anyone used it? How does it compare to other UV materials that
are out
	on the market today?
	
	Thank you,
	
	
	
	
	
	?LeighAnn Litavis
	
	
	
	---------------------------------------------------
	Technet Mail List provided as a service by IPC using LISTSERV
15.0 To
	unsubscribe, send a message to [log in to unmask] with following
text in
	the BODY (NOT the subject field): SIGNOFF Technet To temporarily
halt or
	(re-start) delivery of Technet send e-mail to [log in to unmask]:
SET
	Technet NOMAIL or (MAIL) To receive ONE mailing per day of all
the
	posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the
	archives of previous posts at: http://listserv.ipc.org/archives
Please
	visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
	additional information, or contact Keach Sasamori at
[log in to unmask] or
	847-615-7100 ext.2815
	-----------------------------------------------------
	
	---------------------------------------------------
	Technet Mail List provided as a service by IPC using LISTSERV
15.0 To
	unsubscribe, send a message to [log in to unmask] with following
text in
	the BODY (NOT the subject field): SIGNOFF Technet To temporarily
halt or
	(re-start) delivery of Technet send e-mail to [log in to unmask]:
SET
	Technet NOMAIL or (MAIL) To receive ONE mailing per day of all
the
	posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the
	archives of previous posts at: http://listserv.ipc.org/archives
Please
	visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
	additional information, or contact Keach Sasamori at
[log in to unmask] or
	847-615-7100 ext.2815
	-----------------------------------------------------
	
	---------------------------------------------------
	Technet Mail List provided as a service by IPC using LISTSERV
15.0
	To unsubscribe, send a message to [log in to unmask] with
following text in
	the BODY (NOT the subject field): SIGNOFF Technet
	To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
	To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
	Search the archives of previous posts at:
http://listserv.ipc.org/archives
	Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
	-----------------------------------------------------
	
	


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2