TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Swanson <[log in to unmask]>
Date:
Thu, 18 Sep 2008 09:58:07 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"Douglas O. Pauls" <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (195 lines)
I would generally agree with Peter, but the degree of protection is very 
much an "it depends" proposition.   We use 1B31 here and have for a long 
time.  I did to evaluations of Dymax 984 a number of years ago, and I am 
sure the 9481 has advanced from when I did that testing 7 years ago.   But 
one of the things that I found was that the material was a blend of epoxy, 
acrylic, and urethane polymers.  It gave almost bulletproof for chemical 
resistance, had excellent adhesion, but when we did thermal cycling, we 
had lots of cracking and peeling around the -55C and -65C extremes, a 
place where UV cures have historically had problems.  We also found the 
material to be very hard to rework.

Again, I have not tested the 9481, but if you have to work in worlds below 
-40C, or reworkability is important, then work that into your evaluation 
plan.

Doug Pauls
Rockwell Collins



Peter Swanson <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
09/18/2008 08:18 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Peter Swanson <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] NEW! DUAL-CURET 9481 ELECTRONIC CONFORMAL COATING






Humiseal 1B31 is a single part, solvented acrylic coating, which "dries"
(solvent evaporation) fully in about 1-7 days at room temperature,
depending.  Solvented acrylic coatings are very popular and widely used,
in my experience.

In general terms, you will get more robust protection from a coating
which fully cross-links, and this often means adding external energy
(heat or light, etc). 

Selection of the optimal coating depends on a number of factors,
including operating temperatures and working environments, customer
specifications, electrical characteristics, reworkability and even
production volumes and required process speed. No one coating is
necessarily better than another; horses for courses.

Regards,
Peter

--------------------------------------------------------
Peter Swanson           [log in to unmask]
INTERTRONICS                http://www.intertronics.co.uk
Tel: +44 1865 842842                   Oxfordshire, England

INTERTRONICS is dedicated to providing quality material, consumable 
and equipment solutions to the high technology, high performance 
assembly industries, incorporating outstanding levels of technical 
support and customer service.

Read our news! http://www.intertronics.co.uk/blog/blog.htm

-----Original Message-----
From: Reuven Rokah [mailto:[log in to unmask]] 
Sent: 18 September 2008 14:06
To: TechNet E-Mail Forum; Peter Swanson
Subject: RE: [TN] NEW! DUAL-CURET 9481 ELECTRONIC CONFORMAL COATING

Hi Peter,

Can you compare it with the 1B31?

Best Regards

Reuven ROKAH
e mail: [log in to unmask]
P Think green before printing this mail... Thanks


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Swanson
Sent: Thursday, September 18, 2008 11:40 AM
To: [log in to unmask]
Subject: Re: [TN] NEW! DUAL-CURET 9481 ELECTRONIC CONFORMAL COATING

DYMAX 9481 is a single part acrylated urethane conformal coating. It has
a secondary moisture cure mechanism (a bit like the cure mechanism of a
single part RTV silicone) for those areas which are in shadow to light.
The primary cure mechanism is still UV/visible light.

Traditional UV acrylic conformal coatings had a secondary thermal cure,
so that's what makes this product new - if a secondary cure is required,
there is no need to add heat, the moisture cure just happens over time.

There are similar products from other vendors. This type of chemistry is
a valid choice to evaluate for your coating requirements, but much
depends on board geometry, application methods, requirements of cured
material, etc.

Regards,
Peter

--------------------------------------------------------
Peter Swanson           [log in to unmask]
INTERTRONICS                http://www.intertronics.co.uk
Tel: +44 1865 842842                   Oxfordshire, England

INTERTRONICS is dedicated to providing quality material, consumable and
equipment solutions to the high technology, high performance assembly
industries, incorporating outstanding levels of technical support and
customer service.

Read our news! http://www.intertronics.co.uk/blog/blog.htm

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leigh-Ann Litavis
Sent: 18 September 2008 01:10
To: [log in to unmask]
Subject: [TN] NEW! DUAL-CURE(tm) 9481 ELECTRONIC CONFORMAL COATING

 Hi Technetters,

Can anyone give me some information on this new Dynmax material? Has
anyone used it? How does it compare to other UV materials that are out
on the market today?

Thank you,





?LeighAnn Litavis



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2