I would second Richard, I don't believe the Cu balls are formed the same way as solder, so it would be impossible they contain voids. Could you check with the manufacturer if the ball forming is prone to voiding?
Ioan
-----Message d'origine-----
De : Stadem, Richard D. [mailto:[log in to unmask]]
Envoyé : 18 septembre 2008 09:12
À : [log in to unmask]
Objet : Re: [TN] Copper BGA balls
On those types of components, the copper ball shows up like a void. If
you have a good X-ray and you turn up the magnification, the "void" is
actually a light shade of gray, but not as white as a real void.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Wednesday, September 17, 2008 6:01 PM
To: [log in to unmask]
Subject: [TN] Copper BGA balls
Anyone have experience with components using a tinned copper ball
instead of a SAC alloy solder ball?
Have you ever X-rayed one?
We are seeing voiding that does not meet the IPC-7095B spec for incoming
inspection with a transmission x-ray. However, we don't know if this is
a concern for this type of ball, or if this spec even applies to this
type of ball. I don't think these are meant to collapse and mix with
the solder on the board, like a normal solder alloy ball might.
Once again, thanks in advance for sharing your knowledge.
Genny
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|