TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"McGlaughlin, Jeffrey A" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, McGlaughlin, Jeffrey A
Date:
Mon, 11 Aug 2008 16:17:24 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (94 lines)
Try Cirexx International. You can contact Morgan Hite
([log in to unmask]) at phone number 1-800-217-0202. He has been a good
resource for me in the past.

Jeffrey A McGlaughlin, CID


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Greig
Sent: Monday, August 11, 2008 3:55 PM
To: [log in to unmask]
Subject: [TN] Multilayer Flex-Rigid Fabricators capable of the following

Hi Technet

Apologies for asking what may not be a relevant or appropriate topic for
advice on, but here goes...

I am looking for a fabricators for industrial product volumes (100 per

month) of a troublesome PCB.

4 layer rigid + 2 layer flex + 4 layer rigid, 3 sections with 90 degree
folds. 10 layers total.

Because of large 0.8mm BGA's with > 500 balls I will be looking for:

#1 - 0.25mm(10mil) dia drills, 0.125mm(5mil) annulus on the inner rigid
layers, 0.225mm(9mil) drill wall to adjacent copper
clearances on the inner rigid layers, there will be no copper on the
inner flex in these regions.

#2 - 0.1mm(4mil) track/gap on the inner rigid and 0.125mm(5mil)
track/gap on the outer rigid.

#3 - the flex is only for connections between the main sections and will
be in the form of a microstrip construction, 0.15mm
track/gap(6mil) 45ohm to 60ohm @ 1GHz.

#4 - flex distance board-board < 6mm(1/4inch) with <3mm(1/8inch) radius
@ 90degree, one time bend and mount.

#5 - Need full lead free assembly which will need to withstand at least

4 reflow passes @ 260C

#6 - Service life will be multiple 40C temperature cycles, in excess of
4000 cycles/annum.

#7 - Prefer not to have any acrylic adhesives or bondply, unless the is
data to support their suitability to the reflow
processing.

#8 - UL certs would be a bonus, but could work around this.

#9 - Typical materials might be 370HR and Pyralux AP

It's a for cost constrained imaging/metrology system. To put it in
perspective, the component BOM cost for FPGA's, memories,
DSP, 1.3Mpixel image sensor and laser etc is ~$180 in 100 off
quantities. For that I am getting more than 20billion multiply
adds per second and 2Gbyte of fast memory.

Best Regards

David Greig

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2