We use Huntsman Araldite 8703 daily on many products. It is described as
"overall room temperature curing epoxy system for potting and encapsulation
of electrical and electronic components requiring flame retardancy."
Easy to use - dispense out of a meter-mix system into squirt bottles.
Products are potted in molds and cured by air in a dry box.
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
-----Original Message-----
From: Ken Bloomquist [mailto:[log in to unmask]]
Sent: Tuesday, August 05, 2008 2:38 PM
To: [log in to unmask]
Subject: Re: [TN] Looking for Potting Compound guidance
Hi Carl,
I'm not sure of the cost but at the last company I worked for we used
Emerson and Cuming 2850 FT for potting electronic modules for aircraft. It
worked really well and wasn't too bad to work with.
KennyB
-----Original Message-----
From: Carl VanWormer [mailto:[log in to unmask]]
Sent: Tuesday, August 05, 2008 10:34 AM
To: [log in to unmask]
Subject: [TN] Looking for Potting Compound guidance
Our customer has requested that our product be "potted" to help it survive
longer in an "automotive" environment. Our module is in a plastic box
(black ABS, 80 degree C), and controls a small diesel engine in an enclosed
area. I'm looking for suggestions for a good potting compound that is:
1. "right for the job"
2. low cost
3. easy to use
4. not hazardous
5. makes sense to use in relatively small batches (100 units at 5 ounces
each)
Can any TechNetters suggest potting compounds that they are happy with?
Fatherly guidance and old war stories will be greatly appreciated.
Thanks,
Carl
Carl Van Wormer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR 97006
Phone (503)-617-7447 extension 20
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|