The plating on the PCB is tin lead. The plating on the module is clear chromate. The mechanical use Acetone to clean the module, dried before passing them to me for PCBA assembly.
ESS is at -40C to +85C for 25 cycles. There is no condensation according to the thermal group performing the ESS as compressed air is pumped in the chamber.
Thanks and Regards,
~ Wee Mei ~
________________________________
From: TechNet on behalf of Kevin Glidden
Sent: Mon 8/18/2008 8:36 PM
To: [log in to unmask]
Subject: Re: [TN] Stain Mark after ESS
Couple of things I would check......
Are you certain the PCB finish is tin lead? Make sure what you received is
what you specified.
Could be dissimilar metals issue. What is the module material and finish?
What materials are being used to clean before assembly? Are they adequately
rinsed and dried prior to ESS?
What are the ESS parameters and is condensation occurring?
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
-----Original Message-----
From: Lum Wee Mei [mailto:[log in to unmask]]
Sent: Saturday, August 16, 2008 1:23 AM
To: [log in to unmask]
Subject: [TN] Stain Mark after ESS
Hello,
Prior to assembly the PCBAs onto the modules, inspection has been done to
confirm there is no presence of stain around mounting holes for either
modules or PCBAs. However, after ESS when the PCBAs are removed from the
module to be conformal coated, black stain marks are noticed around the
mounting holes for modules and PCBAs. All PCBAs have a perimeter of tin-lead
plating to provide effective grounding between PCBA and module.
The mechanical group has ensure all modules are thoroughly cleaned before
the assembly. What would be the cause of the black stain and is there any
long-term reliability issue? The mech group has tried using Acetone to
removed the stain but without any success.
Looking forward to your reply and thanks in advance.
Thanks and Regards,
~ Wee Mei ~
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|