You mean he was not?!
--------------------------
Sent using BlackBerry
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Fri Aug 01 09:27:41 2008
Subject: Re: [TN] Solder Paste with craters.
I loved it, but you know people will be saying that poor Inge has gone
over to the dark side. He is using Deweyisms.
Dewey
-----Original Message-----
From: Inge [mailto:[log in to unmask]]
Sent: Thursday, July 31, 2008 2:32 PM
To: Whittaker, Dewey (EHCOE); TechNet E-Mail Forum
Subject: Re: [TN] Solder Paste with craters.
not for a scan dinavian
Inge
----- Original Message -----
From: "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
To: "TechNet E-Mail Forum" <[log in to unmask]>; "Inge"
<[log in to unmask]>
Sent: Thursday, July 31, 2008 2:30 PM
Subject: RE: [TN] Solder Paste with craters.
Yeah, but those clay tablets and papyrus reeds are hard to scan.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Thursday, July 31, 2008 2:27 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Paste with craters.
Mike is too young, and he is english..............
????????????
You didn't know? Most reports, as far as I remember, were american.
IBM,
ESL, HERAUS, duPONT, Honeywell, etc
Inge
----- Original Message -----
From: "John Burke" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, July 31, 2008 2:14 PM
Subject: Re: [TN] Solder Paste with craters.
> If you want REALLY old papers on Rheology Mike Fenner will
have/remember
> them - sorry Mike!!...........NOT
>
>
>
> John Burke
>
> (408) 515 4992
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
> Sent: Thursday, July 31, 2008 1:52 PM
> To: [log in to unmask]
> Subject: Re: [TN] Solder Paste with craters.
>
> Leif Erik,
>
> seems as the focus is now on the stencil. Good, because this may be
the
> red
> thread. Imagine the squeege has just passed and the extremly small
laser
> cut
>
> holes are filled with your paste. Next, the stencil is ready to
separate
> from the board. What happens? I guess the rather rough metal walls are
> little unwilling to let go the paste, while the paste has already
> established a grip on the ENIG pad through surface wetting and
adhesion
> forces. The later one wins over the adhesion from the stencil walls
> (otherwise, there had been no prints). However, the adhesion from the
> walls
> will expand or elongate the paste body for fractions of a second. But
the
> true volume is constant still, isn't it. Then a compensation must be
done,
> namely, the middle of the paste body must sink. You get a small , what
> shall
>
> I call it, a inward bend instead of a flat paste surface. When the the
> stencil wall adhesion is overcome, the paste glides backward and
leaves
> the
> stencil, but not as a perfect cube or cylinder, but more like a
volcano
> crater. What happens next is all dependent on the rheology of the
paste.
> We
> found that pastes with little lower viscosity never gave any bubbles,
> while
> 'thicker' or 'drier' pastes had a tendency to build a 'depression' in
the
> middle. This was only seen for very small apertures. In our case, we
> could
> ignore the phenomenon, didn't have any negative impact. We learned
this
> all
>
> from our thickfilm printing guy. Wished I had saved all hundreds of
> technical report from the 60s and 70s (it was the time we had people
who
> knew about rheology) but they are gone. Later generations thought this
old
> stuff was useless, a lot not even stored for the IT age... Trike Man
may
> still have something hidden in his drawers,,,
>
> Inge
>
>
>
> ----- Original Message -----
> From: "Inge" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Wednesday, July 30, 2008 2:21 PM
> Subject: Re: [TN] Solder Paste with craters.
>
>
>> Do you use a thick stencil?
>> Have you tried to slow down the stencil lift speed?
>>
>> Inge
>>
>>
>> ----- Original Message -----
>> From: "Leif Erik Laerum" <[log in to unmask]>
>> To: <[log in to unmask]>
>> Sent: Wednesday, July 30, 2008 1:56 PM
>> Subject: Re: [TN] Solder Paste with craters.
>>
>>
>>> Thank you everyone for contributing. Especially you, Richard.
>>>
>>> First of all these are NOT via in cap boards and we are using FR4.
Been
>>> there done that....
>>>
>>> Most of the items brought up by Richard we do have established
processes
>>> for. These are according to the recommendations of the solder
vendor,
>>> but
>
>>> if others feel differently, please chime in.
>>> We log the solder used for each batch and the Date of Manufacture
for
>>> this. We typically do not accept a batch of solder that is older
than 3
>>> mts. This is so that we do not end up with too much out of date
solder
>>> at
>
>>> the end.
>>>
>>> - Solder is brought out of the fridge minimum 12 hours before use.
>>> - We set a time limit that solder must can be stored out of the
fridge a
>>> maximum of 3 mts. Practically this ends up around 1 month max.
>>> - We do reuse solder that has been on the screen for up to two
weeks.
>>> Then we throw it out.
>>> - We never put solder back in the fridge.
>>> - We are evaluating new suppliers of solder at the moment. We have
not
>>> audited the currents supplier, but that is a good idea. We always
get
>>> the
>
>>> solder couriered locally and in a cool container so I do not
have
>>> any evidence that would lead me to put this on the solder vendor,
>>> but.....
>>> - As our process works boards sit no longer than 1 hour with solder.
>>> Usually much shorter than that.
>>> - We are using Type 5 solder actually.
>>> - All misprints go though the wash before it is reprinted.
>>> - We use a DEK 248 that is not as automatic as I would like and some
of
>>> the issues we see are due to this repeatability problem, but from
the
>>> data I have gathered, this is not the cause of the solder fines and
>>> craters.
>>> - A Solder AOI would be nice. We do not have one of these (yet???)
>>> - There could be an issue with too much solder. We are going to
reduce
>>> apertures some. There is some evidence of excessive solder.
>>> - I am going to experiment with slowing down the print separation
speed.
>>> Good point.
>>>
>>> Thx.
>>>
>>> Leif Erik Laerum
>>> Quality Assurance Manager
>>> Texas Memory Systems
>>> [log in to unmask]
>>> Tel: (713) 266-3200 x468
>>> www.texmemsys.com
>>>
>>>
>>>
>>> Inge wrote:
>>>> Hi Leif, you've just listened to His Master's Voice.
>>>> You should take off your cap, when you speak to Richard Stadem.
>>>> Impressive! I begin to feel that there are two exceptional stars at
TN.
>>>> Steve...we already knew
>>>> Richard...a supernova
>>>>
>>>> Inge
>>>>
>>>> Gah...my example was not very clever...a supernova is bright just
for
>>>> a
>
>>>> short time...hmmm...a red giant then? hmmm...or a white
>>>> dwarf...hm...none of them very striking....hmm....shining like
>>>> Betelgeuse...hmm.....maybe Master Whittaker can give a hand?
>>>>
>>>>
>>>> ----- Original Message ----- From: "Stadem, Richard D."
>>>> <[log in to unmask]>
>>>> To: <[log in to unmask]>
>>>> Sent: Wednesday, July 30, 2008 6:53 AM
>>>> Subject: Re: [TN] Solder Paste with craters.
>>>>
>>>>
>>>> Hi, Leif
>>>> Send your pictures to [log in to unmask]
>>>>
>>>> Can you tell me what solder paste it is you are using? How was it
>>>> qualified for use?
>>>>
>>>> Here are just some of the questions you need to ask yourself in
order
>>>> to
>>>> determine why you have an issue with solder fines:
>>>> Do you have a good documented solder paste handling procedure? How
is
>>>> the paste handled, from vendor or distributor to your factory? When
was
>>>> the last time you stopped in at the distributor to verify their
stock
>>>> is
>>>> being rotated and is kept refrigerated immediately upon receipt
from
>>>> the
>>>> factory? How often do they turn the packages upside down to prevent
>>>> flux
>>>> separation? Are they a certified distributor who will pass on to
you a
>>>> lot recall notice from your solder paste vendor if there is a known
bad
>>>> lot?
>>>> How long is the paste allowed to sit out on the stencil and how
many
>>>> times can a line of paste on the stencil be sheared (printed back
and
>>>> forth) before it is removed and replenished with fresh paste? Are
the
>>>> operators allowed to scrape up the unused paste on the stencil and
>>>> re-deposit it into a jar for re-use later? Is the jar or tube of
solder
>>>> paste, once removed from refrigeration, allowed to set for two to
four
>>>> hours (depending on paste vendor and paste type) to reach room
>>>> temperature prior to printing? Once removed from the refrigerator,
is
>>>> unused solder paste allowed to be put back in the refrigerator? Are
you
>>>> using Type 4 paste or Type 3? How good is the printer setup, ie,
the
>>>> repeatability of the registration of the stencil to the PWB? Are
you
>>>> performing some type of aperture reduction on all pads in general
and
>>>> at
>>>> least a 50% reduction on large belly pads to prevent solder fines
from
>>>> being printed onto the board? If a board is misprinted, does the
>>>> operator know better than to simply wipe off the board (embedding
the
>>>> paste into every space between the edges of the pads and the
>>>> soldermask,
>>>> into every small via, into every through hole, etc.) but is there a
>>>> documented procedure detailing how the misprinted board is to be
>>>> cleaned
>>>> to prevent this? How is the solder paste packaged, jar or tube?
(Tubes
>>>> prevent a much larger volume of paste from being exposed to air and
>>>> humidity, and also help prevent re-use of solder paste that has
been
>>>> out
>>>> for awhile). Do you perform a good solder paste print inspection
using
>>>> a
>>>> 3d AOI or some other type of automated inspection, and do you use
the
>>>> data from this inspection process to detect (real-time) paste
defect
>>>> trends and react to them with corrective actions?
>>>>
>>>> Sorry to ask so many questions, but all of these can contribute to
>>>> fines, and there are many more factors that can cause them.
>>>>
>>>>
>>>>
>>>> -----Original Message-----
>>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Leif Erik
Laerum
>>>> Sent: Wednesday, July 30, 2008 8:29 AM
>>>> To: [log in to unmask]
>>>> Subject: [TN] Solder Paste with craters.
>>>>
>>>> Technetters,
>>>>
>>>> We are having an issue with solder fines on our lead free boards.
We
>>>> are
>>>> using SAC305 WS and no nitrogen. I noticed that our boards have
craters
>>>> in the paste on the pads after being printed. Not all pads are
>>>> deposited
>>>> this way, but maybe 25%. These craters have an air bubble in them.
The
>>>> bubbles usually burst before the boards goes into the P&P, but the
>>>> crater stays. The screening process is exactly the same for leaded
and
>>>> unleaded paste. The leaded paste does not behave this way. Could
these
>>>> craters be a symptom of the cause of the solder fines? Anyone have
any
>>>> experience with this?
>>>>
>>>> How do I go about posting pictures to stevezeva.homestead.com?.
>>>>
>>>>
>>>> --
>>>> Leif Erik Laerum
>>>> Quality Assurance Manager
>>>> Texas Memory Systems
>>>> [log in to unmask]
>>>> Tel: (713) 266-3200 x468
>>>> www.texmemsys.com
>>>>
>>>> ---------------------------------------------------
>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
To
>>>> unsubscribe, send a message to [log in to unmask] with following text
in
>>>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily
halt
>>>> or
>>>> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>>>> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>>>> posts: send e-mail to [log in to unmask]: SET Technet Digest Search
the
>>>> archives of previous posts at: http://listserv.ipc.org/archives
Please
>>>> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
>>>> additional information, or contact Keach Sasamori at [log in to unmask]
or
>>>> 847-615-7100 ext.2815
>>>> -----------------------------------------------------
>>>>
>>>> ---------------------------------------------------
>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>> To unsubscribe, send a message to [log in to unmask] with following
text
>>>> in
>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>> To temporarily halt or (re-start) delivery of Technet send e-mail
to
>>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>> To receive ONE mailing per day of all the posts: send e-mail to
>>>> [log in to unmask]: SET Technet Digest
>>>> Search the archives of previous posts at:
>>>> http://listserv.ipc.org/archives
>>>> Please visit IPC web site
>>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>>> information, or contact Keach Sasamori at [log in to unmask] or
>>>> 847-615-7100
>
>>>> ext.2815
>>>> -----------------------------------------------------
>>>>
>>>> ---------------------------------------------------
>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>> To unsubscribe, send a message to [log in to unmask] with following
text
>>>> in
>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>> To temporarily halt or (re-start) delivery of Technet send e-mail
to
>>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>> To receive ONE mailing per day of all the posts: send e-mail to
>>>> [log in to unmask]: SET Technet Digest
>>>> Search the archives of previous posts at:
>>>> http://listserv.ipc.org/archives
>>>> Please visit IPC web site
>>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>>> information, or contact Keach Sasamori at [log in to unmask] or
>>>> 847-615-7100
>
>>>> ext.2815
>>>> -----------------------------------------------------
>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following
text
>>> in
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to
>>> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at:
>>> http://listserv.ipc.org/archives
>>> Please visit IPC web site
>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>> information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
>>> ext.2815
>>> -----------------------------------------------------
>>>
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following
text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>
>> for additional information, or contact Keach Sasamori at
[log in to unmask]
>> or
>
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
[log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
[log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|