Unless you make very simple, thin PCBs the change is highly recommended.
However, Tg is not the whole story, you also should choose a material with a
Td(5%) of >= C and a thermal expansion TE(50<=>260C) of <=3.2% . Generally,
you should pick a material with an STII>=215 [the STII combines the effects of
Tg, Td and TE].
If you want to get some background and other suggestions, I would recommend
you get my White Paper: "Recommendations for PCB FAB Notes and Specifications
in Printed Circuit Board Drawings for SnPb and Lead-Free Soldering Assemblies,
the Qualification of PCB Shops and Activities to Assure Continued Quality.
Werner
Future workshops:
Reliability Issues with Lead-Free Soldering Processes, September 22,
Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture,
ENIG), September 22, Schaumburg
Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia
Solder Joint Reliability: Part 4, Oct. 17, Timisoara, Rumania
Solder Joint Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia
**************
Looking for a car that's sporty, fun and fits in your budget?
Read reviews on AOL Autos.
(http://autos.aol.com/cars-Volkswagen-Jetta-2009/expert-review?ncid=aolaut00030000000007 )
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|