FYI: looks like it is a high lead related issue - probably in a move to
comply with RoHS - by adding lead to the bumping process..?????
Quote:
"What supports the theory that a high-lead solder bump in fact is at fault
is the fact that Nvidia ordered an immediate switch to use eutectic solders
instead of high-lead versions in the last week of July. Eutectic solders are
believed to solve the problem of fatigue cracking."
Link is here:
http://www.tomshardware.com/news/Nvidia-GPU-failure,6248.html
Kind regards,
John Burke
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------