Subject: Re: [TN] Smear and rework failure
Hi Pradeep,
NO, smear will not form uniformly.
YES, smear will affect the quality and reliability of the PCBs at every
stage
of subsequent work and operational use.
THEREFORE, effective desmear is a must.
HOWEVER, that does not mean that you need a lot of positive etchback,
because
that too degrades quality and reliability.
You need to be aware that desmearing Pb-free soldering compatible PCB
base
materials, typically phenolic cured, do not respond to smear removal
like the
traditional FR-4 PCBs.
All of this, and of course much more, is detailed in my White Paper
"Recommendations for PCB FAB Notes and Specifications in Printed Circuit
Board Drawings
for SnPb and Lead-Free Soldering Assemblies, the Qualification of PCB
Shops
and Activities to Assure Continued Quality."
Werner
Future workshops:
Reliability Issues with Lead-Free Soldering Processes, September 22,
Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle
Fracture,
ENIG), September 22, Schaumburg
Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia
Solder Joint Reliability: Part 4, Oct. 17, Timisoara, Rumania
Solder Joint Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia
**************
Looking for a car that's sporty, fun and fits in your budget?
Read reviews on AOL Autos.
(http://autos.aol.com/cars-BMW-128-2008/expert-review?ncid=aolaut0005000
0000017 )
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|