Pre-heat is key. I have a Hakko FR1012 that has paid for itself many times
over in situations like yours. Check out:
http://www.hakkousa.com/detail.asp?PID=4211&Page=1
----- Original Message -----
From: "Luan Nguyen" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, August 26, 2008 9:26 PM
Subject: [TN] solder vertical fill on thermal pad
Dear All,
we are having a problem about hand soldering (lead-free) for some PTH parts
mounted on thermal pad. Solder vertical fill is difficult to up 75%. Can you
help us some conditions and technics related for this problem.
Thanks
***************************
Nguyen Hoang Luan
QC&Training Supervisor
Spartronics VietNam Co, Ltd.
No.3, Street No.6, VSIP
Th An Dist., BDuong Prov., VN
Tel: (84-650) 784 890
Fax: (84-650) 784 891
Mobile: 090.3.667448
Email: [log in to unmask]
***************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|