I discovered that the link as shown in the e-mail didn't work, so here is the working link.
http://www.acqp2.nasa.gov/projects/NASA_DODLeadFreeElectronics_Proj2.html
Phil
-----Original Message-----
From: Miller, Michael (Mick) P CIV NSWC Crane, GXSP [mailto:[log in to unmask]]
Sent: Thursday, August 21, 2008 5:25 PM
To: Phil Nutting
Subject: RE: [TN] Compatibility of Lead-Free alloys
Phil,
The answer is the usual, "It depends!" Actually there is not much
PUBLICLY available data on this that I know of, however, the NASA-DOD
Lead-free Electronics Project, aka JG-PP Project 2, is looking at some
of these Lead-free alloy rework compatibility issues. This data, once
collected and analyzed, will be publicly available. Currently the
project is in the final stages of test vehicle fabrication. Then the
rework will need to be performed (estimated to be completed by the
middle of October) and then the testing conducted (estimated to be
started before the end of the calendar year). If you want more
information about the project you can find it at the following website
link:
http://www.acqp2.nasa.gov/projects/NASA_DODLeadFreeElectronics_Proj2.htm
l which gives the project coordinator's, Kurt Kessel, contact
information.
Although I receive the TN posting I cannot reply, so feel free to
forward my reply to TN.
Thank you,
Mick Miller
Crane Division, Naval Surface Warfare Center (NSWC Crane)
Harnessing the Power of Technology for the Warfighter
Printed Circuit Technology Branch, Code GXSP
Ofc: 812-854-5732
FAX: 812-854-1174
DSN 482
-----Original Message-----
From: May, William D (Dean) CIV NSWC Crane, GXSP
Sent: Wednesday, August 20, 2008 11:16 AM
To: Ferguson, Jason D CIV NSWC Crane, GXSP; Mcatee, Edward A CIV NSWC
Crane, GXSP; Brock, Ronald J CIV NSWC Crane, GXSP; Sherfick, Joseph L
CIV NSWC Crane, GXSP; Miller, Michael (Mick) P CIV NSWC Crane, GXSP;
McQueen, Matthew T CIV NSWC Crane, GXSP; Mcdaniel, Martin D CIV NSWC
Crane, GXSP; Vetter, Steve J CIV NSWC Crane, GXSP
Subject: FW: [TN] Compatibility of Lead-Free alloys
-------------------------------------------
From: TechNet on behalf of Phil Nutting[SMTP:[log in to unmask]]
Sent: Wednesday, August 20, 2008 11:13:13 AM
To: [log in to unmask]
Subject: [TN] Compatibility of Lead-Free alloys Auto forwarded by a Rule
Hi all,
In a discussion today the question came up "Is there an issue with using
one lead-free alloy to build a board and a different lead-free alloy to
rework the same board?"
I was under the impression that most lead-free alloys were compatible
with each other with maybe the exception of the ones with bismuth.
I know there are reams of data about tin/lead mixed with lead-free, but
what about SN100C with SAC305 or SN995e?
Phil
Note: All the information contained in this e-mail and its attachments
is proprietary to Kaiser Systems, Inc. and it may not be reproduced
without the prior written permission of sender. If you have received
this email in error, please immediately return it to sender and delete
the copy you received.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|