Leo,
Could they just be illustrating that the finish can withstand 150 C/1000 as an extreme environment and still be "X %" good [in whatever characteristic they were discussing] - and not attempting to tie it into any specific equivalent condition??
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lin Leo
Sent: Friday, August 22, 2008 8:24 AM
To: [log in to unmask]
Subject: [TN] Pre-condition
Hi,
Recently, I got a metal finish-ENEPIG presentation material from vendor. In that presentation, it shows a pre-condition 150 C/1000 hr baking . Why use that baking condition? What working condition or storage does it mean?
Best regards
Leo
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. [gntx v.1]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|