I am curious to know how it will be addressed by the Task groups. As a
board
fabricator, I have my two cents.
Blind vias will be flat and cap plated only if required by customer. In
that
case, separate via fill step using Peters or PHP900 is taken prior to
final
lamination. That is the best way to ensure a flat and platable surface.
If not specified, blinds vias will be filled by resin during final
lamination, the surface will have a concave shape. And depends on
several
factors, the %of fill varies. Then it comes to Electroless copper or
direct
metallization. Electroless copper is very poor at covering the resin
surface, thus the separation or lack of coverage of cap plating. Direct
metallization does better jobs on bare resin spots but not every shop
has
that process.
Regards,
Jason Zhao
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Thursday, August 21, 2008 11:18 AM
To: [log in to unmask]
Subject: Re: [TN] Via hole fill
These issues are being worked and addressed in the Task groups. I know
you've had your fill of this, but it depends.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eddie Rocha
Sent: Thursday, August 21, 2008 8:32 AM
To: [log in to unmask]
Subject: Re: [TN] Via hole fill
Does the 6012B mention anything about blind vias that have a plated cap?
When a blind via falls in an outerlayer ground plane area, it will be
plated
over. I've seen some cross-sections that show separation between that
plated
cap and the resin that filled the blind via hole. Is this covered in
6012B?
Is this a defect?
thanks,
Eddie
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Grunde Gjertsen
Sent: Wednesday, August 20, 2008 11:23 PM
To: [log in to unmask]
Subject: Re: [TN] Via hole fill
Hi
The copper thickness requirement is the same but there is a minimum fill
requirement for blind and buried vias. The plating requirements is
listed
in 6012B table 3-2, the fill requirement is stated in 3.6.2.16, beware
that for space and military avionics the requirements are tighter.
br
Grunde
Scott Westheimer <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
19.08.2008 09:51
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Scott Westheimer <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Via hole fill
Can someone be so kind as to direct me to the IPC specification that
covers filled via's. I am looking for the min average copper plating
thickness required. These are non-conductive filled via's.
Thanks in advance.Scott B. Westheimer5709 Clarks Fork DriveRaleigh, NC
[log in to unmask]: (919)713-0748Cell NC: (919)961-5364
_________________________________________________________________
Get ideas on sharing photos from people like you. Find new ways to
share.
http://www.windowslive.com/explore/photogallery/posts?ocid=TXT_TAGLM_WL_
Phot
o_Gallery_082008
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|