Hi GA,
We measure Young's Modulus on FR4 PWBs with DMA. Our sense is that
repeated thermal excursions associated with lead-free changes Young's
modulus. There appears to be a hysteresis induced by thermal excursions
associated with assembly so I would expect elasticity to be changing
with each thermal excursion.
We do not test assembled boards but the bare circuit board is definitely
changed by thermal excursions associated with lead-free assembly. We see
plastic deformation due to those thermal excursions in our
microsections. We think the plastic deformation relieves internal PWB
stress to some degree, but may induce stress in surface mounted
components. We know that delamination reduces the stress within the
printed wire board. We assume this stress relieves surface mount
components to some degree but have no experience in that area.
A good study would be to associate PWB reliability to changes in Young's
modulus due to the thermal excursion associated with tin-lead and
lead-free assembly. We have not done these studies yet but I expect they
would be informative. If the PWB is getting stiffer with each thermal
excursion, I expect more stress to be induced in the internal
interconnections and mounted components.
Sincerely,
Paul Reid
Program Coordinator
PWB Interconnect Solutions Inc.
235 Stafford Rd., West, Unit 103
Nepean, Ontario
Canada, K2H 9C1
613 596 4244 ext. 229
Skype paul_reid_pwb
[log in to unmask] <mailto:[log in to unmask]>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tan Geok Ang
Sent: Wednesday, August 13, 2008 9:11 PM
To: [log in to unmask]
Subject: [TN] Elasticity
Hi All,
Can the elasticity of FR4 rigid PCB and solder joints
(SnPb, SAC) be definite (with value)? Thanks in advance.
Best Regards
GA Tan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|