Edward Szpruch
Manager of Process Engineering
Eltek Ltd
[log in to unmask] | www.eltekglobal.com
Tel: +972 3 939 5098 | Fax: +972 3 930 9581 |Cell: +972 54 8074298
P נא להימנע מלהדפיס מסמך זה על נייר במידת האפשר
Hi,
It seems to me,that the phrase " too much Phosphorus (> 7%) can lead to "Black Pad" is a modern version of the " too much sex makes your eyes going crasy" - it used to be very popular poster in late sixties.
Edward
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete Houwen
Sent: Wednesday, August 27, 2008 3:53 PM
To: [log in to unmask]
Subject: Re: [TN] ENIG & BORON
"I know that too much Phosphorus (> 7%) can lead to "Black Pad". "
Actually, the occurance of Black Pad has become far less frequent since the
introduction of Hi-P nickel baths, with about 9%-13% P. It's now more a
matter of process control than P content.
---------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|