Hi all
Need advise. This has happenned twice in the last 2 months. The battery
leaked all over the card (S-M - CNC 45 card no. 45.01.02.3) The m/cs did not
start the next day.
If the card is powered after a few years of storage the battery starts
leaking and within a few days it is all over the PCB.
We removed the chips and cleaned in Hot water / air agitn and againa nd
again. Baked bare card and reloaded chips. NADA. Solvent extarct of bare PCB
all perfect.
Advise if we should change all chips - some TTL, some cmos, memory, eproms,
etc.
Anil
Micro Interconnexion Pvt. Ltd
D3-12 A, Corlim Ind. Estate
Corlim, ILHAS, GOA
INDIA - 403110
Tel: +91-832-2284337
Fax: +91-832-2284209
alt. E-mail: [log in to unmask]
LEADERS IN GOLD PLATED PCBs
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------