TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Date:
Wed, 27 Aug 2008 08:34:54 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bill Coleman <[log in to unmask]>
Subject:
From:
Bill Coleman <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
Hi Kane

Photo Stencil manufactures both Laser-Cut and Electroform step stencils.  The normal step keep-out design guides are found in IPC 7525.  35 mils per mil of step thickness is recommended as keep out for apertures in the 3 mil area to the step-up to 5 mils.  25 mils keep-out from the step-down to 3 mils to an aperture in the 5 mil thick area.

Regards, 

William E. Coleman Ph.D. 
Vice President Technology 
Phone: 719-535-8528 
Cell:     719-331-2433 
Fax:     719-599-4334 

 

CONFIDENTIALITY NOTICE: This e-mail transmission, and any documents, files or previous e-mail messages attached to it, may contain confidential information that is legally privileged. If you are not the intended recipient, or a person responsible for delivering it to the intended recipient, you are hereby notified that any disclosure, copying, distribution or use of any of the information contained in or attached to this message is STRICTLY PROHIBITED. If you have received this transmission in error, please immediately notify us by telephone at (719) 599-4305 and destroy the original transmission and its attachments without reading them or saving them to disk. Thank you.







-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Kane, Amol (349)
Sent: Wednesday, August 27, 2008 8:27 AM
To: [log in to unmask]
Subject: [TN] FW: Step Stencil Requirements


_____________________________________________
From: Kane, Amol (349)
Sent: Wednesday, August 27, 2008 8:13 AM
To: [log in to unmask]
Subject: Step Stencil Requirements


Dear Technetters,
I am looking for some information about using step stencils in production. I have a 16 mil pitch QFN component with 7.8 mil square pads. This gives me unacceptable area ratio using a 5 mil stencil. Looks like I am going to have to use a 3 mil thick stencil with this component. I was thinking of using a 5 mil stencil with a 3 mil step.  There are chip components around the QFN device. The board is Lead-Free with ENIG finish. Using a Type 4 solderpaste.

I was looking for inputs from folks who are using step stencils on the squeegee types (metal vs. poly), changes in print parameters (speed, pressure, Snap off etc,), board design considerations (keep out areas around the component needing the step), resources I could go thru to obtain more information, stencil houses who specialize in this process, and common pitfalls.

Any inputs will be greatly appreciated.

Thanks,
Amol





WARNING:  Export Control 
This document may contain technical data within the definition of the 
International Traffic in Arms Regulations (ITAR), and subject to the Export 
Control Laws of the U.S. Government.  Transfer of such data by any means to a 
foreign person, whether in the United States or abroad, without proper export 
authorization or other approval from the U.S. Department of State is 
prohibited. 
 
CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy 
all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2