Tue, 26 Aug 2008 19:02:42 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Willis <[log in to unmask]>
Subject:
From:
Bob Willis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (140 lines)
Thanks to Bill for the comments on Breakfast, the best ever solder finish
with a unique benefit was developed for cooking equipment, particularly for
woks.

The finish offered by Panasonic on single sided boards was cockroach
repellent. 

www.bobwillis.co.uk/pdf/cockroachcoating.pdf

Now there is a good one to liven up your next solder finishes seminar, it
features in my Basic PCB Manufacture Workshop and always gets a laugh.





Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
 
www.ASKbobwillis.com
 
New Bob Willis "Printed Board Inspection & Quality Control Workshop" 3rd
September www.ASKbobwillis.com/PCBworkshop.pdf 
 
Book your place on Bob's "Step by Step Failure Analysis Workshop" 11th
September  www.ASKbobwillis.com/faworkshops.pdf
 
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: 26 August 2008 13:25
To: [log in to unmask]
Subject: Re: [TN] ENIG White paper

Hi, Bob
Dave stated he was looking for a flat finish, thus his desire to move to
ENIG. We were simply pointing out that an IAg flat finish is more often
preferable than ENIG. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Willis
Sent: Tuesday, August 26, 2008 1:51 AM
To: [log in to unmask]
Subject: Re: [TN] ENIG White paper

There have been many comments on this subject but few asking why move
away from HASL or do you not want to use tin/lead or lead-free HASL?

There are lots of high end users that have found good PCB shops who are
able to provide a good repeatable surface finish. Its key to work with
your supplier and lead-free works well for solderability and assembly
yields.

Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
 
www.ASKbobwillis.com
 
New Bob Willis "Printed Board Inspection & Quality Control Workshop" 3rd
September www.ASKbobwillis.com/PCBworkshop.pdf 
 
Book your place on Bob's "Step by Step Failure Analysis Workshop" 11th
September  www.ASKbobwillis.com/faworkshops.pdf
 
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Connitt
Sent: 21 August 2008 19:06
To: [log in to unmask]
Subject: [TN] ENIG White paper

Dear Technetters,
 
I am trying to locate a white paper on the pluses and minuses of ENIG
that I think was circulated through the IPC. Can anyone point me to that
document? We are considering changing from HASL to ENIG for our SMT
designs and want to see what we should look for or anticipate.
Thanks,
Dave Connitt

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2