You have not stated what type of component is being affected and how
many. Has this ever happened be before on the vendor in questioned. A
photo is worth one thousands words.
Vic,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ted Tontis
Sent: Monday, August 25, 2008 9:49 AM
To: [log in to unmask]
Subject: Re: [TN] Cracked component leads
I am looking to rule out the possibility that the crack is further then
the
tin plating. I am pulling parts off the reel that have what appears to
be a
crack in the terminal. We are also seeing a large number of assemblies
with
severed leads after the wave process. The supplier is telling me that it
is
the plating that is cracked not the lead. I hope that after dyeing, the
lead
can be broken off and the penetration of dye measured. If it penetrates
the
copper then I know the crack is deeper then the tin plating.
Thank you,
Ted
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Monday, August 25, 2008 9:37 AM
To: [log in to unmask]
Subject: Re: [TN] Cracked component leads
Once you have done your dye penetrant what means/technique will you use
to determine how far and what direction the suspected crack propagated.?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|