Hi Dave,
The workshop you are looking for is PD-01:Solder Joint Reliability: Failure
Mode and Root Cause Analyses (Fatigue, Brittle Fracture, ENIG) on Sept. 22,
2008 9:00 to 12:00. If you do a Keyword search under "ENIG," it comes up.
Under 'time bomb' I mean that you may be sitting on a supply of PCBs waiting
to be needed, only to find out when you are assembling them that you have a
problem—of course, if they are properly manufactured you may not, but you do not
know.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
**************
It's only a deal if it's where you want to go. Find your travel
deal here.
(http://information.travel.aol.com/deals?ncid=aoltrv00050000000047)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|