TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 22 Aug 2008 16:04:16 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob METCALF <[log in to unmask]>
Subject:
From:
Bob METCALF <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (117 lines)
I would also be very interested to see data that suggest ENIG properly 
processed by the fabricator is a potential time bomb. My experience has 
always been that ENIG that has had problems can be traced back to improper 
processing at the fabricator. 

Regards,

Bob Metcalf
Atotech Western Regional Manager

Cell 714-334-7667
E-Mail [log in to unmask] 

This e-mail and any attachments hereto are business documents of Atotech 
USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS INFORMATION. 
Unauthorized disclosure and/or use of information contained in this email 
is prohibited. If you are not the intended recipient, you may not read, 
use, disseminate or copy this message or any other files transmitted with 
it. 



Dave Connitt <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
08/21/2008 01:37 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] ENIG White paper






Werner,
That's interesting.. Is there any data on that you could refer me to?
Dave Connitt 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: Thursday, August 21, 2008 4:30 PM
To: [log in to unmask]
Subject: Re: [TN] ENIG White paper

Hi Dave,
Based on my experience, ENIG is more of a (time)-bomb than imAg.


Werner
Future workshops:
Reliability Issues with Lead-Free Soldering Processes, September 22, 
Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle
Fracture, 
ENIG), September 22, Schaumburg
Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia
Solder Joint Reliability: Part 4, Oct. 17, Timisoara, Rumania
Solder Joint Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia



**************
It's only a deal if it's where you want to go. Find your travel 
deal here.
 
(http://information.travel.aol.com/deals?ncid=aoltrv00050000000047)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2