Leland, forgot to tell you that not all resistor chips are for uwave
applications.
there ARE chips intended for mounting with resistor print against the board,
e.g.
http://www.caddock.com/Online_catalog/Mrktg_Lit/TypeCHR.pdf
Inge
----- Original Message -----
From: "Inge" <[log in to unmask]>
To: "TechNet E-Mail Forum" <[log in to unmask]>; "Leland Woodall"
<[log in to unmask]>
Sent: Thursday, July 31, 2008 3:28 PM
Subject: Re: [TN] Repair Need for Inverted Chip Resistors
> There are two or three reasons not to turn them up and down (if you are a
> microwave guy >1 GHz ):
>
> 1. The L-cut laser trim groove may be filled by active substances from the
> flux. (no glass or paint overprint)
> 2. We have done simulations which show that your insertion and return loss
> may be disadvantageous.
> 3. None of our suppliers have demonstrated anything else than print side
> up.
>
> E.g. Anaren, one of our good sources
>
> http://www.anaren.com/content/File/AnarenCeramicsDesignGuide.pdf
>
> Inge
>
>
> ----- Original Message -----
> From: "Leland Woodall" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Thursday, July 31, 2008 12:11 PM
> Subject: Re: [TN] Repair Need for Inverted Chip Resistors
>
>
> Dewey and others,
>
> I've been told the concern lies with the resistive element being on top
> of the component. With it being mounted upside down, the hottest
> portion of the part when under power is in direct contact with the
> board. Would this lead to shortened life or cause any type of a
> premature failure?
>
> Are we being over-cautious about this, or is there some truth to what
> I'm being told?
>
> Leland
>
> -----Original Message-----
> From: Whittaker, Dewey (EHCOE) [mailto:[log in to unmask]]
> Sent: Thursday, July 31, 2008 2:00 PM
> To: TechNet E-Mail Forum; Leland Woodall
> Subject: RE: [TN] Repair Need for Inverted Chip Resistors
>
> I'll try to be discreet. If there is no functional impact, then a "let
> the chips fall where they may" approach is acceptable. If the part
> markings are not visible or the vision recognition algorithm of an AOI
> machine is impaired, then they may be a problem.
> Dewey
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
> Sent: Thursday, July 31, 2008 10:12 AM
> To: [log in to unmask]
> Subject: [TN] Repair Need for Inverted Chip Resistors
>
> TechPros,
>
> Can anyone tell me if there's a reliability concern with allowing chip
> resistors to be mounted upside down? Our current policy requires that
> we repair these, and I feel that to be unnecessary.
>
> IPC-A-610D shows this to be an acceptable condition on all classes of
> product, and our customer has no specific contractual requirement.
>
> I'd like to try to change this policy at our facility, and welcome any
> commentary you might have on the subject.
>
> Thanks in advance for your help,
>
> Leland Woodall
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|