Vladimir
Here are potential causes of MLCCC cracking, and how to tell what caused
the crack based on the crack's position, run direction, etc.
http://www.ami.ac.uk/courses/topics/0179_fmcc/index.html#3
http://www.syfer.com/category_docs/AN0005_Mechanical_Cracking.pdf
And an authorative paper on the subject by John Maxwell, who I think
knows more about root causes of cap cracking than anyone:
http://www.avx.co.il/docs/techinfo/cracks.pdf
And a potential solution to the problem:
http://www.avx.co.il/docs/techinfo/mlccflex.pdf
Qualify it first.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir
Sent: Monday, July 14, 2008 1:13 PM
To: [log in to unmask]
Subject: Re: [TN] Ceramic caps
Well, in the case I was asking about none of the failures were in that
direction (across the body) but always along it splitting both ends in
half either vertically or horizontally. Still a puzzle to me :-)
Regards,
Vladimir
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Monday, July 14, 2008 2:05 PM
To: [log in to unmask]
Subject: Re: [TN] Ceramic caps
Right!
KennyB
-----Original Message-----
From: Igoshev, Vladimir [mailto:[log in to unmask]]
Sent: Monday, July 14, 2008 10:48 AM
To: TechNet E-Mail Forum; Ken Bloomquist
Subject: RE: [TN] Ceramic caps
So they were cracking normal to, not along the body of the caps. Right?
Regards,
Vladimir
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|