Totally understand.
The MLCCCs are in a sort of laminated configuration, with the capacitive
plates stacked on top of dialectrics. They vary depending on the value,
ie, the higher the capacitance, the more layers and the thinner/thicker
the dielectric in between each one. As a result, I know that higher
values of capacitance have more of a tendency to fracture with a lateral
delamination than smaller capacitance values do (I think I said that
correctly). Are the caps that are fracturing all of the same value?
-----Original Message-----
From: Igoshev, Vladimir [mailto:[log in to unmask]]
Sent: Monday, July 14, 2008 1:55 PM
To: TechNet E-Mail Forum; Stadem, Richard D.
Subject: RE: [TN] Ceramic caps
I know Steve would do it, but I need a permission form the "local
authorities" so to say :-)
Regards,
Vladimir
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, July 14, 2008 2:49 PM
To: [log in to unmask]
Subject: Re: [TN] Ceramic caps
Vladimer, if you have photos you can email them to Steve Gregory. Steve
is a gentleman and a scholar of the industry who posts photos so all of
us can see, then it is easier to make a "root cause" analysis or just a
WAG.
Steve's email address is [log in to unmask]
-----Original Message-----
From: John Maxwell [mailto:[log in to unmask]]
Sent: Monday, July 14, 2008 1:44 PM
To: TechNet E-Mail Forum; Stadem, Richard D.
Subject: Re: [TN] Ceramic caps
Richard & Vladimir,
It would be helpful to post the photos and then I can comment.
John Maxwell
> Vladimir
> Here are potential causes of MLCCC cracking, and how to tell what
> caused the crack based on the crack's position, run direction, etc.
> http://www.ami.ac.uk/courses/topics/0179_fmcc/index.html#3
>
> http://www.syfer.com/category_docs/AN0005_Mechanical_Cracking.pdf
>
> And an authorative paper on the subject by John Maxwell, who I think
> knows more about root causes of cap cracking than anyone:
>
> http://www.avx.co.il/docs/techinfo/cracks.pdf
>
> And a potential solution to the problem:
>
> http://www.avx.co.il/docs/techinfo/mlccflex.pdf
>
> Qualify it first.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir
> Sent: Monday, July 14, 2008 1:13 PM
> To: [log in to unmask]
> Subject: Re: [TN] Ceramic caps
>
> Well, in the case I was asking about none of the failures were in that
> direction (across the body) but always along it splitting both ends in
> half either vertically or horizontally. Still a puzzle to me :-)
>
> Regards,
>
> Vladimir
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|