IPC-D-300G 'Printed Board Dimensions and Tolerances'
3.2.3 Unsupported Hole Diameters as
Fabricated:Drilled,Molded,Perforated,etc
3.2.4 Plated-Through Hole (PTH), Finished Diameter.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Wednesday, July 09, 2008 12:12 PM
To: [log in to unmask]
Subject: Re: [TN] Flex specifications - tolerance on hole size
Hi Joe
Agreed. I'm somewhat amused that there is such a split on the
interpretation of this - all valid viewpoints, and some very strongly
held.
The one big lesson from these replies - they do illustrate the need for
clear drawing notes.
regards,
- Graham
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Wednesday, July 09, 2008 12:56 PM
To: [log in to unmask]
Subject: Re: [TN] Flex specifications - tolerance on hole size
Everyone who has commented is basically right based on their varying
perspectives.
Providing a tolerance on a via is not necessary for accept or reject,
so long as it has the copper needed/requested but it is important to
know what is happening on internal layers and therein lies the rub.
It is very helpful for the designer to know something about the
manufacturing process and manufacturing tolerances to avoid painting
themselves into a corner (which happens more often than should be) and
wasting time with after the fact clarifications.
Time spent with a manufacture learning about the process before
designing is time well spent.
Joe
In a message dated 7/9/2008 7:33:47 A.M. Pacific Daylight Time,
[log in to unmask] writes:
I tend to recommend keeping the fab print to reflect the "finished" PCB
requirements. That way the inspectors have a "black and white" document
to inspect the PCBs too throughout the fab process. If the process
attributes were specified they might change depending on which factory
and where they are made. Those could be written up in a Customer
Specification document that is separate than the fab print but chances
are there would be a series of waivers/deviation requests between the
fabricator and OEM.
Cheers,
Groovy (aka, Dave Hoover)
----- Original Message -----
From: "Barton, Ken" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, July 09, 2008 7:19 AM
Subject: Re: [TN] Flex specifications - tolerance on hole size
If we started dialing in the drill sizes for actual drill size before
plate
as opposed to finished (plated) size, it would surely confuse the heck
out
of our fab houses.
Ken Barton
-----Original Message-----
From: John Burke [mailto:[log in to unmask]]
Sent: Tuesday, July 08, 2008 4:28 PM
To: [log in to unmask]
Subject: Re: [TN] Flex specifications - tolerance on hole size
The hole size MUST be the drilled size. If it is NOT the drilled size
you
have no control whatsoever over the design in terms of drill to copper
clearances. If you must call out a finished hole size do it separately
on
the drawing for the holes concerned.
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Tuesday, July 08, 2008 8:45 AM
To: [log in to unmask]
Subject: Re: [TN] Flex specifications - tolerance on hole size
Hey guys.
Thanks for all the opinions and info. I'm stuck in the middle, on one
side is a designer saying that it means pre-finishing size, on the
other
I've got a fabricator saying it means finished hole size. The drawing
is ambiguous on this point. I just want parts to build things with!!!
I do agree with Werner that it does not matter as they are only vias,
but once someone had inspected and measured something it became a
debate.
regards,
- Graham
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Monday, July 07, 2008 7:57 PM
To: [log in to unmask]
Subject: Re: [TN] Flex specifications - tolerance on hole size
Hi Werner,
I like your thinking but...
I'm not in the quality department, no offense to those of you who are,
but I wouldn't want to be ;-) But thinking like an inspector, how would
you verify that you got the right size holes if you don't call out a
finished hole size? I guess you could do a cross section but a pin gage
is a lot simpler.
Just thinking out loud,
KennyB
-----Original Message-----
From: Werner Engelmaier /* [mailto:[log in to unmask]]
Sent: Monday, July 07, 2008 3:36 PM
To: [log in to unmask]
Subject: Re: [TN] Flex specifications - tolerance on hole size
Hi Graham,
Why do you care what the finished hole size is? Do you put component
leads into 0.028"/+- 0.003" holes, that is 25 mils minimum?
The finished hole size specifications are an anachronism harking back
to
the
THT-days-today they only should be specified for componet lead holes.
For vias the drilled hole diameter should be specified-it is much more
important.
Werner
Future workshops:
Pb-Free Soldering Processes-Survival, Quality, Reliability, July 17/18,
Thal, Switzerland Pb-Free Soldering Processes-Survival, Quality,
Reliability, July 21/22, Bad Segeberg, Germany Pb-Free Soldering
Processes-Survival, Quality, Reliability, August 18, Orlando
Reliability
Issues with Lead-Free Soldering Processes, September 22, Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle
Fracture,
ENIG), September 22, Schaumburg
Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia Solder
Joint Reliability: Parts 1 & 4, Oct. 17, Timisoara, Rumania Solder
Joint
Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
**************Get the scoop on last night's hottest shows and the live
music
scene in your area - Check out TourTracker.com!
(www.tourtracker.com?NCID=aolmus00050000000112)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|