TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Eric Kalgren <[log in to unmask]>
Date:
Wed, 2 Jul 2008 13:41:16 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mike Sewell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Mike Sewell <[log in to unmask]>
Parts/Attachments:
text/plain (197 lines)
We had blacklight bulbs in the spray room and under the booth/hood to
aid the sprayer with coverage checking.  The intensity wasn't high
enough to cure overspray very quickly, but would cure it over several
hours.  If you make pallets that fit in you UV oven then you could cure
both at the same time and not have to handle a wet board directly. You
can cover a reusable pallet with paper or even have them cut out of
corrugated cardboard if you want to throw them away. 

Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric Kalgren
Sent: Wednesday, July 02, 2008 12:18 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coating Waste

How about a hanging blacklight?  I bought some standard sized bulbs to
fit a
shop fluorescent light fixture a while back.  They used to be readily
available at your neighborhood big box home improvement store.  You
could
hang it in a vented fume hood in an isolated area to cure and vent any
fumes.

Or you could get your hands on a tanning bed and provide tanning as an
employee perk when you're not curing your coating waste!

Eric Kalgren
Electrical Engineer
The Ferrite Co. Inc.
165 Ledge Street
Nashua, NH 03060
Phone 603-881-5234
Fax 603-881-5406
 
 
PRIVILEGED AND CONFIDENTIAL COMMUNICATION
This E-mail is covered by the Electronic Communications Privacy Act, 18
U.
S. C." 2510-2521 and is legally privileged.  The information contained
herein is confidential and is intended only for the use of the
individual or
entity named above.  If the reader of this message is not the intended
recipient, you are hereby notified that any dissemination, distribution
or
copying of this communication is strictly prohibited.  If you have
received
this transmission in error, please immediately notify the sender by
telephone or via e-mail and delete the original transmission including
any
attachments without reading or saving in any manner. 
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Wednesday, July 02, 2008 1:11 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coating Waste

Yes,
Same here in upstate NY (maybe not so much right now).......I would end
up
with a bunch of snow on them 5 months from now!

Amol


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Wednesday, July 02, 2008 11:23 AM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coating Waste

Hi Amol,

We don't use UV coating so it's not an issue but I was wondering if you
could put the paper out in the sun for a little bit. Of course here in
Western Washington that would be a problem since we never get any sun
;-)

KennyB

-----Original Message-----
From: Kane, Amol (349) [mailto:[log in to unmask]]
Sent: Wednesday, July 02, 2008 6:17 AM
To: [log in to unmask]
Subject: [TN] Conformal Coating Waste

Dear Technetters,
We regularly use absorbent paper to rest the boards in the conformal
coating
booth as we spray them (UV cure coatings). A question came up recently
about
the paper being hazardous waste due to uncured coating on it. I want to
know
if:
1. Anybody else is using a similar method to coat the boards and how is
disposal being handled
2. Is there an alternative to using paper in the coating booth. The
disposal
issue will still remain

I do not want to put the paper in the UV oven for curing.

Any advice will be greatly appreciated.

Thanks,
Amol


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------



WARNING:  Export Control 
This document may contain technical data within the definition of the 
International Traffic in Arms Regulations (ITAR), and subject to the
Export 
Control Laws of the U.S. Government.  Transfer of such data by any means
to
a 
foreign person, whether in the United States or abroad, without proper
export 
authorization or other approval from the U.S. Department of State is 
prohibited. 
 
CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy

all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2