We are experiencing poor solderability with AgPd-terminations on MOVs
exposed to a lead-free reflow profile using a SAC alloy on an
ENIG-finished PCB. Though we have run this board only once previously
with the same part finish using a lead-rich alloy, we had similar
effects but not to the extent we are now experiencing.
Can anyone provide some insight into this/
Regards
Grant
**********************************************************************
Relevant company disclaimers are available at the following addresses:
Tellumat (Pty) Ltd e-mail: mailto:[log in to unmask]
Web: http://www.tellumat.com/email.aspx
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------