Edding 751 paint pens
Use 4 dots of 4 colours gives about 256 numbers (I think)
And it won't come off in normal operation, passes through reflow and can
be read (normally)
Rex
Rex Waygood
Technical Manager
Tel: +44 (0)1202 674333
Fax: +44 (0)1202 678028
DDI: +44 (0)1202 338222
Mob: +44 (0)7887 997403
[log in to unmask]
www.PartnerTech.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: 17 July 2008 15:35
To: [log in to unmask]
Subject: [TN] Indelible marking
Dear Technos,
I need to serialize about 200 BGAs (simply write on them sequential
numbers 1-200). The BGAs will be assembled, SnPb process with water
soluble flux, then washed in plain water in our in-line washer.
In case the customer will not accept us scratching the numbers onto the
top of the components, what kind of permanent ink can I use?
And would you see any issue with scratching the top of the components?
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
-------------------------------------------------------------------------------
The information contained within this e-mail and any attachments contained therein may be confidential and/or legally privileged and is for the use of the intended recipient only. If you are not the intended recipient please delete it from your system and notify the sender by return e-mail. The content of this e-mail may not be copied or disclosed to any third parties without prior permission from the sender.
E-mail is susceptible to data corruption, interception, tampering and viruses. We do not accept any liability for any such incidents or any consequences thereof.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|