Looking for some advice on how to handle a new bottom only termination
device we have. We don't normally run devices with bottom only
terminations, so the inspection has not been an issue, until now. Any
recommendations on how to inspect these, or verify the process is working?
I am thinking I might process some samples and send them to a lab for
x-sections (we do not have x-section capability here). Is that sufficient?
Thanks in advance!
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------