Hi Patricia,
You can find it on IPC-4552 (spec for ENIG for PCBs). It is min. 2 u" for
gold. 118 to 236 u" for Nickel
Jackson Chan
Technical Services Manager
Cookson Electronics - Alpha Metals (Hong Kong)
Low cost, reliable alloy SACX0807
Patricia Lui
<[log in to unmask]
.SG> To
Sent by: TGAsia [log in to unmask]
<[log in to unmask]> cc
Subject
2008/07/25 ¤U¤È [TGA] Immersion gold thickness
04:04 enquiry
Please respond to
Asia Committe
Task Group Forum
<[log in to unmask]>;
Please respond to
Patricia Lui
<[log in to unmask]
.SG>
Dear Friend,
Did IPC indicate that immersion gold thickness have to be minimum 2u" gold?
This 2u" thickness is referring to the gold thickness only or it is the
total thickness which includes the nickel too? Which IPC documents
indicates this?
Hope to have your expertise advise.
Thanks & Best Regards
Patricia Lui
Xuan Technology LLP.
email: [log in to unmask]
Search. browse and book your hotels and flights through Yahoo! Travel