Are these via-in-pad boards?? Crater in same spot on each pad - not random.
Denny Fritz
MacDermid
-----Original Message-----
From: Guy Ramsey <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, 30 Jul 2008 12:31 pm
Subject: Re: [TN] Solder Paste with craters.
I have not see that kind of print anomaly. Obviously this will change the
solder volume and it is undesirable. While the craters are not causing the
fines. They could be symptomatic of a failure in the material that results
in fines.
The flux should dry and then the solder coalesce onto the feature at reflow.
Some pastes fail in so that the flux runs all over carrying the solder
spheres with it off the pads. Then at reflow the flux burns off leaving
fines stranded everywhere.
I have run into this problem and I have receive bad solder paste from
reputable suppliers that do this fresh from a sealed jar.
You could observe this with a BGA rework station, hot air or IR pen. Compare
the problem paste with fresh paste and paste that does not produce fines.
I think you will see a difference.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, July 30, 2008 11:59 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Paste with craters.
Hi Leif!
I have your pictures posted. Go to:
http://stevezeva.homestead.com/files/air_bubbles_and_craters_1.jpg
http://stevezeva.homestead.com/files/air_bubbles_and_craters_2.jpg
Is the percentage of metals the same as your leaded paste? I also think the
rheology the paste won't be the same with as it is with the leaded paste, so
there will most likely have to be changes with the set-up of the print. It
almost looks like the separation speed is too fast, and the paste isn't
given time to pull away from the inside of the apertures causing the
crater...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leif Erik Laerum
Sent: Wednesday, July 30, 2008 8:29 AM
To: [log in to unmask]
Subject: [TN] Solder Paste with craters.
Technetters,
We are having an issue with solder fines on our lead free boards. We are
using SAC305 WS and no nitrogen. I noticed that our boards have craters in
the paste on the pads after being printed. Not all pads are deposited this
way, but maybe 25%. These craters have an
air bubble in them. The bubbles
usually burst before the boards goes into the P&P, but the crater stays. The
screening process is exactly the same for leaded and unleaded paste. The
leaded paste does not behave this way. Could these craters be a symptom of
the cause of the solder fines? Anyone have any experience with this?
How do I go about posting pictures to stevezeva.homestead.com?.
--
Leif Erik Laerum
Quality Assurance Manager
Texas Memory Systems
[log in to unmask]
Tel: (713) 266-3200 x468
www.texmemsys.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------
------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|