A braided stainless Celtic weave tongue stud? (ewww)
At 07:25 AM 6/5/2008, Bev Christian wrote:
>A hair net? Just kidding.
>Bev
>RIM
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
>Sent: Thursday, June 05, 2008 10:15 AM
>To: [log in to unmask]
>Subject: [TN] Stainless Steel Contamination Question - Source Nailed!
>
>Everyone,
>
>After checking every filter, every transfer belt, every reflow oven, and
>most every square inch of the building, I was able to identify the
>source of the 10 micron stainless steel that has been giving us such a
>headache. Just in case anyone ever has the same problem, I thought I'd
>share the solution with our group.
>
>To refresh your memory, we were finding this stuff on top of components,
>and later inside our Huntron X-Y table inspection machines. We did
>everything but take a hatchet to the Huntrons, and there was nothing
>found (of course).
>
>While one of the Huntron machine's operator was gone to lunch, I decided
>to check an item she had left behind on her workstation. I took it to
>the lab, placed it beneath the microscope, and was astonished to find an
>identical match to our contamination woes.
>
>Before I let the cat out of the bag, does anyone want to venture a
>guess?
>
>Leland
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------------------------
>This transmission (including any attachments) may contain
>confidential information, privileged material (including material
>protected by the solicitor-client or other applicable privileges),
>or constitute non-public information. Any use of this information by
>anyone other than the intended recipient is prohibited. If you have
>received this transmission in error, please immediately reply to the
>sender and delete this information from your system. Use,
>dissemination, distribution, or reproduction of this transmission by
>unintended recipients is not authorized and may be unlawful.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|