TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Leland Woodall <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Leland Woodall <[log in to unmask]>
Date:
Thu, 5 Jun 2008 10:14:53 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (33 lines)
Everyone,

After checking every filter, every transfer belt, every reflow oven, and
most every square inch of the building, I was able to identify the
source of the 10 micron stainless steel that has been giving us such a
headache.  Just in case anyone ever has the same problem, I thought I'd
share the solution with our group.

To refresh your memory, we were finding this stuff on top of components,
and later inside our Huntron X-Y table inspection machines.  We did
everything but take a hatchet to the Huntrons, and there was nothing
found (of course).

While one of the Huntron machine's operator was gone to lunch, I decided
to check an item she had left behind on her workstation.  I took it to
the lab, placed it beneath the microscope, and was astonished to find an
identical match to our contamination woes.

Before I let the cat out of the bag, does anyone want to venture a
guess?

Leland

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2